Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 190 - 250 µm | 190 - 250 µm | Mean Granulate Size |
Nabaltec GRANALOX® NM 9212 B Ceramic Body, Binder Free Nabaltec offers ceramic bodies with different alumina content as free-of-binder grades. With the addition of necessary amount of water (approx. 20 %) these grades can be directly used for slip casti.. |
|||
Particle Size | 180 - 250 µm | 180 - 250 µm | |
Potters Industries A-Series P-0100 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Particle Size | 150 - 250 µm | 150 - 250 µm | Range |
Potters Industries Spheriglass® 1922 Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |
|||
Particle Size | 0.100 - 250 µm | 0.100 - 250 µm | Average value: 111 µm Grade Count:27 |
Overview of materials for PVC, Powder This property data is a summary of similar materials in the MatWeb database for the category "PVC, Powder". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Particle Size | 63.0 - 250 µm | 63.0 - 250 µm | Average value: 157 µm Grade Count:8 |
Overview of materials for PVC, Uncompounded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Uncompounded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Particle Size | 63.0 - 250 µm | 63.0 - 250 µm | Average value: 155 µm Grade Count:14 |
Overview of materials for PVC, Rigid Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Particle Size | 100 - 250 µm | 100 - 250 µm | |
Lucite International Elvacite ® 4080 Acrylic Resin Elvacite® 4080 is a medium molecular weight methyl methacrylate copolymer. It is a relatively flexible acrylic resin useful for improving the recoatability and intercoat adhesion of UV wood finis.. |
|||
Particle Size | 63.0 - 250 µm | 63.0 - 250 µm | Average value: 157 µm Grade Count:12 |
Overview of materials for PVC, Molded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |