Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 0.100 - 250 µm | 0.100 - 250 µm | Average value: 111 µm Grade Count:27 |
Overview of materials for PVC, Powder This property data is a summary of similar materials in the MatWeb database for the category "PVC, Powder". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |