Polymer Property : Particle Size = 250 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size 190 - 250 µm
190 - 250 µm
Mean Granulate Size
Nabaltec GRANALOX® NM 9212 B Ceramic Body, Binder Free
Nabaltec offers ceramic bodies with different alumina content as free-of-binder grades. With the addition of necessary amount of water (approx. 20 %) these grades can be directly used for slip casti..
Particle Size 180 - 250 µm
180 - 250 µm
Potters Industries A-Series P-0100 Soda-Lime Silica Technical Quality Solid Glass Spheres
Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil..
Particle Size 150 - 250 µm
150 - 250 µm
Range
Potters Industries Spheriglass® 1922 Solid Glass Spheres
Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage..
Particle Size 0.100 - 250 µm
0.100 - 250 µm
Average value: 111 µm Grade Count:27
Overview of materials for PVC, Powder
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Powder". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Particle Size 63.0 - 250 µm
63.0 - 250 µm
Average value: 157 µm Grade Count:8
Overview of materials for PVC, Uncompounded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Uncompounded". Each property range of values reported is minimum and maximum values of appropriate ..
Particle Size 63.0 - 250 µm
63.0 - 250 µm
Average value: 155 µm Grade Count:14
Overview of materials for PVC, Rigid Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M..
Particle Size 100 - 250 µm
100 - 250 µm
Lucite International Elvacite ® 4080 Acrylic Resin
Elvacite® 4080 is a medium molecular weight methyl methacrylate copolymer. It is a relatively flexible acrylic resin useful for improving the recoatability and intercoat adhesion of UV wood finis..
Particle Size 63.0 - 250 µm
63.0 - 250 µm
Average value: 157 µm Grade Count:12
Overview of materials for PVC, Molded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb..