Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | <= 100 µm | <= 100 µm | 90% smaller than |
Nyco MG WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | <= 100 µm | <= 100 µm | 90% smaller than |
Nyco NYAD® MG Wollastonite High aspect ratio grade. This grade is recommended for elastomer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinct.. |
|||
Particle Size | <= 100 µm | <= 100 µm | 90% smaller than |
Nyco NYGLOS® 20 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | <= 100 µm | <= 100 µm | |
Potters Industries A-Series P-0040 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Particle Size | 100 µm | 100 µm | Average Diameter |
Potters Industries Conduct-O-Fil® AG-SL150-16-TRD Silver-coated Hollow Ceramic Spheres Applications: Conductive paints and coatings; Aerospace and other mass-critical applications. Advantages include low density, easily mixed into paint systems, large particle sizeInformation provide.. |
|||
Particle Size | 100 µm | 100 µm | Average Diameter |
Potters Industries Conduct-O-Fil® AG-SL150-30-TRD Silver-coated Hollow Ceramic Spheres Applications: Conductive paints and coatings; Aerospace and other mass-critical applications. Advantages include low density, easily mixed into paint systems, large particle sizeInformation provide.. |
|||
Particle Size | 100 - 175 µm | 100 - 175 µm | D 0.9, SATP-114, Malvern method |
Raschig Group PiMC 1221 High gloss PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa.. |
|||
Particle Size | 100 - 175 µm | 100 - 175 µm | D 0.9, SATP-114, Malvern method |
Raschig Group PiMC 1241 Sanitary, uni color PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa.. |
|||
Particle Size | 100 - 175 µm | 100 - 175 µm | D 0.9, SATP-114, Malvern method |
Raschig Group PiMC 1249 Sanitary, mix color PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa.. |
|||
Particle Size | 100 - 175 µm | 100 - 175 µm | D 0.9, SATP-114, Malvern method |
Raschig Group PiMC 1841 Metallic colors Adding metallic effect pigments to powder coatings gave rise to several application problems such as “spitting”. Synres-Almoco’s Metallic PiMC 1841 ensures easy processing and homogeneous surface.. |
|||
Particle Size | 100 - 175 µm | 100 - 175 µm | D 0.9, SATP-114, Malvern method |
Raschig Group PiMC 1949 Granite colors PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa.. |
|||
Particle Size | 100 - 200 µm | 100 - 200 µm | |
Polimeri Europa Extir® E 5000 AE Expandable Polystyrene
(discontinued **) Extir E 5000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium-large particle size, with a low pentane content as blowing agent. Extir does not contain CFC or H.. |
|||
Particle Size | 100 - 140 µm | 100 - 140 µm | Laser Light Scattering Method; LSY-QB-ID016 |
LG Chemical Lutex 111 NBR Latex Description: Tensile strength, Elongation, Oil resistance, Abrasion resistance, Excellent elasticity, WhitenessApplication: Nitrile Glove (Examination Glove, Clean Room Glove), Supported Glove (Indu.. |
|||
Particle Size | 100 - 150 µm | 100 - 150 µm | Mean particle size is 100 to 150 µm. Crystal size is 10 µm. |
Momentive Performance Materials AC-6028 Boron Nitride (BN) Powder Grade AC-6028 consists of agglomerated particles of hexagonal Boron Nitride (BN) with a mean particle size between 100 and 150µ. It exhibits the unique properties of BN in a form readily used in.. |
|||
Particle Size | 100 - 170 µm | 100 - 170 µm | |
Lucite International Elvacite ® 2614 Acrylic Resin Elvacite® 2614 is a low molecular weight methyl methacrylate / n-butyl methacrylate copolymer. It is a fast – dissolving, low viscosity grade with quick solvent release for use in industrial.. |
|||
Particle Size | 100 - 200 µm | 100 - 200 µm | |
Lucite International Elvacite ® 4045 Acrylic Resin Elvacite® 4045 is a medium molecular weight methyl methacrylate polymer. It is designed for use in solvent based screen printing inks, but can be used in a variety of ink formulations.Information.. |
|||
Particle Size | >= 100 µm | >= 100 µm | >95 |
Solvay Chemicals Ixper® 35M Magnesium Peroxide IXPER® 35M is a Magnesium Peroxide powder used in a wide range of applications in environmental, and oil drilling e.g. markets. EINECS Number: 215-627-7/CAS Number: 1335-26-8Information provided .. |
|||
Particle Size | 100 µm | 100 µm | 95%, Laser diffraction; QSOP-5&75 |
Shamrock Technologies Fluoro T® 702 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Particle Size | 100 µm | 100 µm | 95%, Laser diffraction; QSOP-5&75 |
Shamrock Technologies Fluoro T® 802 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Particle Size | <= 100 µm | <= 100 µm | 3% Max; 540MA3C5E |
Solvay MIRAPOL® SURF-S 411 HA Surfactant Description: Rinse aid polymer specially formulated for auto dish wash powders and tablets. Recommended as a substitute to rinse aid surfactants. Enables raw material cost saving, while boosting rin.. |
|||
Particle Size | 100 µm | 100 µm | 95%, Laser diffraction; QSOP-5&75 |
Shamrock Technologies Fluoro T® 602 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Particle Size | 100 µm | 100 µm | Average Mean |
SPHERE ONE EXTENDOSPHERESâ„¢ PM 6550 Hollow Plastic Spheres PM 6550 PM 6550 is an extremely light and versatile hollow sphere. Its plastic composition results in a very low density product. Only a very small amount of this hollow sphere is needed to provide .. |
|||
Particle Size | >= 100 µm | >= 100 µm | d90, 20%, Vibrated sieving |
TIMCAL TIMREX® KS150 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 100 µm | 100 µm | 98% less than value (Size B) |
Vesta Ceramics SicoMill® Grade 2 Silicon Powder General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu.. |
|||
Particle Size | 100 µm | 100 µm | 98% less than value (Size B) |
Vesta Ceramics SicoMill® Grade 4 Silicon Powder General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu.. |
|||
Particle Size | 100 µm | 100 µm | |
TIMCAL TIMREX® M100 mesh Natural Flake Graphite TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-.. |
|||
Particle Size | 100 - 300 µm | 100 - 300 µm | 0.65 |
Arkema Group OREVAC® 18732 Grafted Maleic Anhydride Polypropylene OREVAC 18732 and 18732P are maleic anhydride grafted polypropylene used in the manufacturing of multiplayer structures. These products are available in pellets or in powder. OREVAC 18732 and 18732P .. |
|||
Particle Size | 100 µm | 100 µm | Average |
Azoty Tarnow™ TARFLEN SM-2 PTFE Non Free Flowing suspension powder for standard compression molding and compounding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Particle Size | 100 - 150 µm | 100 - 150 µm | average |
Momentive Performance Materials PolarTherm® PT350 Boron Nitride (BN) Powder Low Density BN AgglomerateWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic compon.. |
|||
Particle Size | 100 - 150 µm | 100 - 150 µm | |
Potters Industries A-Series P-0060 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |