Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.89 g/cc | 0.321 lb/in³ | |
NiCoForm NiColoy® E Electroformed Nickel-Cobalt NiColoy® is a proprietary electrodeposited Nickel-Cobalt alloy distinguished by the following combination of features:Leveled, smooth matte to semi bright deposit with low internal stressHigh tensi.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
IBC Advanced Alloys C18150 Chrome Copper Zirconium Alloy, TL06 Temper C18150 Chrome Copper Zirconium is recommended for spot and seam welding cold and hot-rolled steel, stainless steel and low conductivity brass and bronze. C18150 Chrome Copper Zirconium Alloy is typi.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
Misumi Z3234 Chromium Copper Excellent mechanical strength and abrasion resistance at high temperatures. Used in welding electrodes, seam welding wheels, switch gears, electrode holder jaws, cable connectors, current carrying a.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | at RT |
Haynes Hastelloy® C-276 alloy, solution heat treated flat products Hastelloy® C-276 alloy is a nickel-molybdenum-chromium wrought alloy that is a versatile corrosion-resistant alloy. C-276 alloy is an improved wrought version of alloy C in that it usually doesn'.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
Special Metals INCONEL® Alloy C-276 A nickel-molybdenum-chromium alloy with an addition of tungsten having excellent corrosion resistance in a wide range of severe environments. The high molybdenum content makes the alloy especially .. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
Special Metals INCONEL® C276 Nickel Superalloy Plate Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed plate. Other property values are typical of INCO® C276.Data provided by the manufacturer, Specia.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
Special Metals INCONEL® C276 Nickel Superalloy Sheet Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed sheet. Other property values are typical of INCO® C276.Data provided by the manufacturer, Specia.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
Special Metals INCONEL® C276 Nickel Superalloy Tubing, 0% Cold Work (Annealed) Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed tubing. Other property values are typical of INCO® C276.Data provided by the manufacturer, Speci.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
Special Metals INCONEL® C276 Nickel Superalloy Tubing, 27% Cold Work Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed + 27% cold worked tubing. Other property values are typical of INCO® C276.Data provided by the m.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
Special Metals INCONEL® C276 Nickel Superalloy Tubing, 30% Cold Work Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed + 30% cold worked tubing. Other property values are typical of INCO® C276.Data provided by the m.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
Special Metals Nickel 200 Commercially pure (99.6%) wrought nickel with good mechanical properties and resistance to a range of corrosive media. Good thermal, electrical, and magnetostrictive properties. Ferromagnetic. Us.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
Special Metals Nickel 270 A high-purity grade of nickel made by powder metallurgy. It has a low base hardness and high ductility. Its extreme purity is useful for components of hydrogen thyratrons. It is also used for ele.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | As Annealed |
Eagle Brass 200/201 Nickel Alloy, 1/4 Hardened Nickel 200/201 has properties that are useful in industries such as chemical processing and electronics. Nickel is resistant to various reducing chemicals and alkaline materials. Compared with nick.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | As Annealed |
Eagle Brass 200/201 Nickel Alloy, 3/4 Hardened Nickel 200/201 has properties that are useful in industries such as chemical processing and electronics. Nickel is resistant to various reducing chemicals and alkaline materials. Compared with nick.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | As Annealed |
Eagle Brass 200/201 Nickel Alloy, Annealed Nickel 200/201 has properties that are useful in industries such as chemical processing and electronics. Nickel is resistant to various reducing chemicals and alkaline materials. Compared with nick.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | As Annealed |
Eagle Brass 200/201 Nickel Alloy, Full Hardened Nickel 200/201 has properties that are useful in industries such as chemical processing and electronics. Nickel is resistant to various reducing chemicals and alkaline materials. Compared with nick.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | Annealed |
Eagle Brass 725 Copper Nickel Tin, 1/4 Hard Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | Annealed |
Eagle Brass 725 Copper Nickel Tin, Annealed Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | Annealed |
Eagle Brass 725 Copper Nickel Tin, Extra Spring Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | Annealed |
Eagle Brass 725 Copper Nickel Tin, Hard Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | Annealed |
Eagle Brass 725 Copper Nickel Tin, Spring Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
CMW® 28 Copper Alloy CMW® 28 material is a copper base alloy having very high electrical and thermal conductivity and medium strength and toughness. It is a heat treatable alloy and develops its strength and hardness t.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
CMW® 3 Copper Alloy CMW® 3 material is a high strength, high conductivity copper base alloy. CMW® 3 material is heat treatable. Optimum mechanical and physical properties of CMW® 3 material are developed by heat tre.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
Cadi 162 Copper Alloy Cadmium addition to copper increases hardness and resistance to softening. C16200 is utilized in numerous applications where fatigue strength and high electrical conductivity are required. Cadmium.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
Cadi 1815 Copper Alloy Zirconium addition to chromium copper improves creep resistance at high operating temperatures and reportedly reduces sticking of electrodes to the work during spot welding of galvanized materials. .. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
California Fine Wire Nickel Alloy 180 Copper Nickel Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
California Fine Wire Nickel Alloy 60 Copper Nickel Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
Carlson C 200 Commercially Pure Nickel General DescriptionCarlson Alloy C 200 is commercially pure nickel, combining good mechanical properties with excellent resistance to many corrosive environments. This alloy retains its strength at.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
Carlson GOC 276 Nickel-Molybdenum-Chromium General DescriptionCarlson Alloy GOC 276 is a nickel-molybdenum-chromium alloy exhibiting outstanding corrosion resistance over a wide range of service environments. This alloy is generally use in .. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
Alloy Wire International RW 45 Ni-Cu Resistance Wire Used in thermocouples, power resistors, shunts, and wire wound precision restors up to 750°F (400°C)Information provided by Alloywire International. |