NiCoForm NiColoy® E Electroformed Nickel-Cobalt

Category Metal , Nonferrous Metal , Nickel Alloy
Manufacturer NiCoForm, Inc.
Trade Name NiColoy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NiCoForm NiColoy® E Electroformed Nickel-Cobalt.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
NiColoy® is a proprietary electrodeposited Nickel-Cobalt alloy distinguished by the following combination of features:Leveled, smooth matte to semi bright deposit with low internal stressHigh tensile strengthMedium-to-high hardnessHigh modulus of elasticityHigh corrosion resistanceHigh purityAmenable to soldering, brazing and welding
Physical Properties Metric English Comments
Density 8.89 g/cc
0.321 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 1100 MPa
160000 psi
ASTM E345-93, Type A Specimen
Tensile Strength, Yield 758 MPa

@Strain 0.100 %
110000 psi

@Strain 0.100 %
ASTM E345-93, Type A Specimen
827 MPa

@Strain 0.200 %
120000 psi

@Strain 0.200 %
ASTM E345-93, Type A Specimen
965 MPa

@Strain 1.00 %
140000 psi

@Strain 1.00 %
ASTM E345-93, Type A Specimen
Elongation at Break >= 1.5 %
>= 1.5 %
ASTM E345-93, Type A Specimen
Elongation at Yield >= 1.0 %
>= 1.0 %
ASTM E345-93, Type A Specimen
Tensile Modulus 122.4 GPa
17750 ksi
ASTM E111-04
Flexural Modulus 165 GPa
23900 ksi
ASTM E855-90, Test Method B
Thermal Properties Metric English Comments
CTE, linear 13.3 µm/m-°C

@Temperature 20.0 - 100 °C
7.39 µin/in-°F

@Temperature 68.0 - 212 °F
ASTM E228-07
Component Elements Properties Metric English Comments
Carbon, C <= 0.10 %
<= 0.10 %
Cobalt, Co >= 1.0 %
>= 1.0 %
Nickel, Ni >= 90 %
>= 90 %
Sulfur, S <= 0.080 %
<= 0.080 %
Descriptive Properties Value Comments
Rockwell Superficial Hardness, HR 15-N 73-83