Material Notes:
C18150 Chrome Copper Zirconium is recommended for spot and seam welding cold and hot-rolled steel, stainless steel and low conductivity brass and bronze. C18150 Chrome Copper Zirconium Alloy is typically used in pencil-type & light soldering guns: tips, rod extensions, resistance welding electrodes, welding electrodes, welding wheels, and tips and rod extensions.Information provided by IBC Advanced Alloys.
Physical Properties Metric English Comments
Density 8.89 g/cc
0.321 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 78 - 82
78 - 82
Plate and Rounds
Tensile Strength 517 - 586 MPa
75000 - 85000 psi
Plate and Rounds
Tensile Strength, Yield 496 - 565 MPa

@Strain 0.200 %
72000 - 82000 psi

@Strain 0.200 %
Plate and Rounds
Elongation at Break 16 %
16 %
Plate and Rounds
Modulus of Elasticity 117 GPa
17000 ksi
Thermal Properties Metric English Comments
CTE, linear 17.1 µm/m-°C
9.50 µin/in-°F
Thermal Conductivity 323.4 W/m-K
2244 BTU-in/hr-ft²-°F
Melting Point 1070 - 1080 °C
1950 - 1980 °F
Solidus 1070 °C
1950 °F
Liquidus 1080 °C
1980 °F
Component Elements Properties Metric English Comments
Chromium, Cr 0.50 - 1.5 %
0.50 - 1.5 %
Copper, Cu 98.25 - 99.45 %
98.25 - 99.45 %
As Balance
Silicon, Si 0.20 - 0.35 %
0.20 - 0.35 %
Zirconium, Zr 0.050 - 0.25 %
0.050 - 0.25 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000200 ohm-cm
0.00000200 ohm-cm
Plate and Rounds