Alloy Wire International RW 45 Ni-Cu Resistance Wire

Category Metal , Nonferrous Metal , Copper Alloy
Manufacturer Alloy Wire International
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Alloy Wire International RW 45 Ni-Cu Resistance Wire.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Used in thermocouples, power resistors, shunts, and wire wound precision restors up to 750°F (400°C)Information provided by Alloywire International.
Physical Properties Metric English Comments
Density 8.89 g/cc
0.321 lb/in³
Thermal Properties Metric English Comments
CTE, linear 14.7 µm/m-°C

@Temperature 20.0 - 100 °C
8.17 µin/in-°F

@Temperature 68.0 - 212 °F
Melting Point 1270 °C
2320 °F
Maximum Service Temperature, Air 400 °C
752 °F
Component Elements Properties Metric English Comments
Copper, Cu 55 %
55 %
Nickel, Ni 45 %
45 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000490 ohm-cm

@Temperature 20.0 °C
0.0000490 ohm-cm

@Temperature 68.0 °F