Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Special Metals INCONEL® C276 Nickel Superalloy Tubing, 0% Cold Work (Annealed)

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer Special Metals (includes the former Inco Alloys International Inc.)
Trade Name INCONEL®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Special Metals INCONEL® C276 Nickel Superalloy Tubing, 0% Cold Work (Annealed).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed tubing. Other property values are typical of INCO® C276.Data provided by the manufacturer, Special Metals.
Physical Properties Metric English Comments
Density 8.89 g/cc
0.321 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 726.7 MPa
105400 psi
Typical
Tensile Strength, Yield 313 MPa

@Strain 0.200 %
45400 psi

@Strain 0.200 %
Typical Annealed
Elongation at Break 70 %
70 %
Typical Annealed
Modulus of Elasticity 205 GPa
29700 ksi
Poissons Ratio 0.307
0.307
Shear Modulus 79.0 GPa
11500 ksi
Thermal Properties Metric English Comments
Specific Heat Capacity 0.427 J/g-°C
0.102 BTU/lb-°F
Thermal Conductivity 9.80 W/m-K
68.0 BTU-in/hr-ft²-°F
Melting Point 1325 - 1370 °C
2417 - 2500 °F
Solidus 1325 °C
2417 °F
Liquidus 1370 °C
2500 °F
Component Elements Properties Metric English Comments
Carbon, C <= 0.010 %
<= 0.010 %
Chromium, Cr 14.5 - 16.5 %
14.5 - 16.5 %
Cobalt, Co <= 2.5 %
<= 2.5 %
Iron, Fe 4.0 - 7.0 %
4.0 - 7.0 %
Manganese, Mn <= 1.0 %
<= 1.0 %
Molybdenum, Mo 15 - 17 %
15 - 17 %
Nickel, Ni 59 %
59 %
As remainder
Phosphorous, P <= 0.040 %
<= 0.040 %
Silicon, Si <= 0.080 %
<= 0.080 %
Sulfur, S <= 0.030 %
<= 0.030 %
Vanadium, V <= 0.35 %
<= 0.35 %
Electrical Properties Metric English Comments
Magnetic Permeability 1.0002
1.0002
at 200 Oersted (15.9 kA/m)