Material Notes:
General DescriptionCarlson Alloy C 6021 is a nickel-chromium alloy, developed specifically for high –temperature service. This alloy exhibits outstanding resistance to both cyclic and static oxidation at temperatures up to 2300°F (1260°C). It has good resistance to aqueous corrosion and high mechanical strength.The high chromium and nickel content of C 601 provide a substantial degree of resistance to carburizing, nitriding and sulfur containing environments. The nickel-base also assures good resistance to stress corrosion cracking.C 601 exhibits excellent tensile and yield strengths and good creep-rupture strength. It will not become embrittled by extended exposure to high temperatures.ApplicationsThermal Processing – baskets, trays and fixtures for annealing, carburizing, carbonitriding, nitriding and other heat treating applications: radiant tubes, muffles, retorts, flame shields and burner nozzles in industrial furnaces; furnace atmosphere generators; infrared radiant shields.Chemical Processing – process heaters and insulating cans in ammonia reformers; combustion components and catalyst grid supports in nitric acid production; catalyst regenerators and air preheaters in polyethylene production.Pollution Control – combustion chambers in solid waste incineratorsPower Generation – superheater tube supports, grid barriers and ash-handling systems.Gas Turbines – containment ringsInformation provided by Carlson
Physical Properties Metric English Comments
Density 8.11 g/cc
0.293 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 552 MPa
>= 80000 psi
Tensile Strength, Yield >= 207 MPa

@Strain 0.200 %
>= 30000 psi

@Strain 0.200 %
Elongation at Break >= 35 %
>= 35 %
Creep Strength 1.379 MPa

@Temperature 1090 °C,
Time 3.60e+7 sec
200.0 psi

@Temperature 2000 °F,
Time 10000 hour
1% creep
4.826 MPa

@Temperature 982 °C,
Time 3.60e+7 sec
700.0 psi

@Temperature 1800 °F,
Time 10000 hour
1% creep
8.9632 MPa

@Temperature 871 °C,
Time 3.60e+7 sec
1300.0 psi

@Temperature 1600 °F,
Time 10000 hour
1% creep
Modulus of Elasticity 206 GPa
29900 ksi
Tension
Poissons Ratio 0.267
0.267
Shear Modulus 81.4 GPa
11800 ksi
Thermal Properties Metric English Comments
CTE, linear 17.1 µm/m-°C

@Temperature 21.1 - 871 °C
9.50 µin/in-°F

@Temperature 70.0 - 1600 °F
Specific Heat Capacity 0.448 J/g-°C
0.107 BTU/lb-°F
Melting Point 1302 - 1368 °C
2375 - 2495 °F
Solidus 1302 °C
2375 °F
Liquidus 1368 °C
2495 °F
Component Elements Properties Metric English Comments
Aluminum, Al 1.0 - 1.7 %
1.0 - 1.7 %
Boron, B <= 0.0060 %
<= 0.0060 %
Carbon, C <= 0.10 %
<= 0.10 %
Chromium, Cr 21 - 25 %
21 - 25 %
Copper, Cu <= 1.0 %
<= 1.0 %
Iron, Fe 7.079 - 19.9 %
7.079 - 19.9 %
Manganese, Mn <= 1.0 %
<= 1.0 %
Nickel, Ni 58 - 63 %
58 - 63 %
Silicon, Si <= 0.50 %
<= 0.50 %
Sulfur, S <= 0.015 %
<= 0.015 %
Titanium, Ti 0.10 - 0.60 %
0.10 - 0.60 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.000119 ohm-cm
0.000119 ohm-cm
Curie Temperature <= -195.56 °C