Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

California Fine Wire Stablohm 710 Nickel Chromium Resistance Wire

Category Metal , Electronic/Magnetic Alloy , Nonferrous Metal , Nickel Alloy
Manufacturer California Fine Wire
Trade Name Stablohm
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF California Fine Wire Stablohm 710 Nickel Chromium Resistance Wire.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Physical Properties Metric English Comments
Density 8.11 g/cc
0.293 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 827 MPa
120000 psi
Annealed
1210 MPa
175000 psi
Stress relieved
1380 MPa
200000 psi
Hard
Thermal Properties Metric English Comments
CTE, linear 12.19 µm/m-°C

@Temperature 20.0 °C
6.772 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 0.460 J/g-°C

@Temperature 20.0 °C
0.110 BTU/lb-°F

@Temperature 68.0 °F
Thermal Conductivity 13.7 W/m-K
95.1 BTU-in/hr-ft²-°F
Melting Point 1377 °C
2511 °F
Maximum Service Temperature, Air 1260 °C
2300 °F
Operating Temperature
Component Elements Properties Metric English Comments
Chromium, Cr 30 %
30 %
Nickel, Ni 70 %
70 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.000118 ohm-cm
0.000118 ohm-cm
3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02
Descriptive Properties Value Comments
Magnetic None
Temperature Coefficient of Resistance 0.000089 ohms/ohm-°C
0-100°C