Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.17 - 1.18 g/cc | 0.0423 - 0.0426 lb/in³ | Polymerized; ASTM D792 |
Proto3000 Objet VeroBlack FullCure870 Rigid Opaque Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Density | 1.17 - 1.18 g/cc | 0.0423 - 0.0426 lb/in³ | Polymerized; ASTM D792 |
Proto3000 Objet VeroGray FullCure850 Rigid Opaque Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Density | 0.900 - 1.18 g/cc | 0.0325 - 0.0426 lb/in³ | Average value: 0.994 g/cc Grade Count:32 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO), Extrusion Grade". Each property range of values reported is mini.. |
|||
Density | 0.0130 - 1.18 g/cc | 0.000470 - 0.0426 lb/in³ | Average value: 0.974 g/cc Grade Count:117 |
Overview of materials for Polystyrene, Molded, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Density | 1.15 - 1.18 g/cc | 0.0415 - 0.0426 lb/in³ | Average value: 1.15 g/cc Grade Count:7 |
Overview of materials for Polycarbonate/Thermoplastic Polyurethane Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Thermoplastic Polyurethane Blend". Each property range of values reported is minimum and m.. |
|||
Density | 1.18 - 1.18 g/cc | 0.0426 - 0.0427 lb/in³ | |
Solvay IGEPAL® CO 210 Surfactant Description: Nonyl phenol ethoxylate (1.5EO). Foam stabilizer (in low concentration) for high-foaming detergents. Defoamer (in higher concentration) for low-foaming and cold-water detergents. Co-em.. |
|||
Density | 1.16 - 1.18 g/cc | 0.0419 - 0.0426 lb/in³ | FTTC 2419 |
Formosa Plastics 35% Hydrochloric Acid Information provided by Formosa Plastics Corporation, USA |
|||
Density | 1.14 - 1.18 g/cc | 0.0412 - 0.0426 lb/in³ | ISO R 1183 |
Fainplast Compounds CTS 55/1 Flexible PVC, Extrusion Modified with Rubber Profiles high elasticity |
|||
Density | 1.14 - 1.18 g/cc | 0.0412 - 0.0426 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 4510/R Flexible PVC, Injection Molding for Footwear Vamp Boots with Rubber |
|||
Density | 1.14 - 1.18 g/cc | 0.0412 - 0.0426 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 55/AT Flexible PVC, Injection Molding for Transparent Technical Items Toys |
|||
Density | 1.14 - 1.18 g/cc | 0.0412 - 0.0426 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 55/KSN Flexible PVC, Injection Molding for Transparent Technical Items Cupping-glasses |
|||
Density | 1.14 - 1.18 g/cc | 0.0412 - 0.0426 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 55/T Flexible PVC, Injection Molding for Footwear Soles |
|||
Density | 1.14 - 1.18 g/cc | 0.0412 - 0.0426 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 55/UV Flexible PVC, Injection Molding for Transparent Technical Items Outdoor protections for switches anti-UV |
|||
Density | 1.14 - 1.18 g/cc | 0.0412 - 0.0426 lb/in³ | ISO R 1184 |
Fainplast Compounds MPH 57/T Medical Flexible PVC, Extrusion Extrusion and injection components no DOP |
|||
Density | 1.14 - 1.18 g/cc | 0.0412 - 0.0426 lb/in³ | ISO R 1184 |
Fainplast Compounds MPH 62/D Medical Flexible PVC, Extrusion Technical tubes no DOP |
|||
Density | 1.14 - 1.18 g/cc | 0.0412 - 0.0426 lb/in³ | ISO R 1183 |
Fainplast Compounds PH 50/1 Flexible PVC, Transparent Extrusion Transparent profiles |
|||
Density | 1.14 - 1.18 g/cc | 0.0412 - 0.0426 lb/in³ | ISO R 1183 |
Fainplast Compounds PH 50/AM-UV Flexible PVC, Transparent Extrusion Gaskets anti mould and anti-UV |
|||
Density | 1.14 - 1.18 g/cc | 0.0412 - 0.0426 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 598A Polyether-based TPU Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech |
|||
Density | 1.15 - 1.18 g/cc | 0.0415 - 0.0426 lb/in³ | Average value: 1.16 g/cc Grade Count:6 |
Overview of materials for Acrylic, Impact Modified Sheet This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified Sheet". Each property range of values reported is minimum and maximum values of.. |
|||
Density | 1.17 - 1.18 g/cc | 0.0423 - 0.0426 lb/in³ | Polymerized; ASTM D792 |
Proto3000 Objet VeroWhitePlus FullCure835 Rigid Opaque Prototyping Polymer Information provided by Proto3000 for their protoyping engineering services. |
|||
Density | 1.14 - 1.18 g/cc | 0.0412 - 0.0426 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 56/R Flexible PVC, Injection Molding for Footwear Oil resistant vamp boots |
|||
Density | 1.14 - 1.18 g/cc | 0.0412 - 0.0426 lb/in³ | ISO R 1183 |
Fainplast Compounds PMP 60 Flexible PVC, Extrusion Modified with PU Various profiles |
|||
Density | 1.14 - 1.18 g/cc | 0.0412 - 0.0426 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 959A Polyether-based TPU Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech |