Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Austin Novel Materials Texalan® 598A Polyether-based TPU

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyether Grade
Manufacturer Austin Novel Materials
Trade Name Texalan®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Austin Novel Materials Texalan® 598A Polyether-based TPU.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech
Physical Properties Metric English Comments
Density 1.14 - 1.18 g/cc
0.0412 - 0.0426 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 95 - 101
95 - 101
ISO 7619
Tensile Strength >= 48.0 MPa
>= 6960 psi
ISO 37
Tensile Stress >= 15.0 MPa

@Strain 100 %
>= 2180 psi

@Strain 100 %
ISO 37
>= 32.0 MPa

@Strain 300 %
>= 4640 psi

@Strain 300 %
ISO 37
Elongation at Yield >= 400 %
>= 400 %
ISO 37
Tear Strength >= 140 kN/m
>= 799 pli
ISO 34
K Factor (Wear Factor) <= 60
<= 60
[mm<sup>3</sup>]; ISO 4649
Compression Set <= 42 %

@Temperature 70.0 °C
<= 42 %

@Temperature 158 °F
ISO 815
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved