Austin Novel Materials Texalan® 959A Polyether-based TPU

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyether Grade
Manufacturer Austin Novel Materials
Trade Name Texalan®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Austin Novel Materials Texalan® 959A Polyether-based TPU.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech
Physical Properties Metric English Comments
Density 1.14 - 1.18 g/cc
0.0412 - 0.0426 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 92 - 98
92 - 98
ISO 7619
Tensile Strength >= 45.0 MPa
>= 6530 psi
ISO 37
Tensile Stress >= 10.0 MPa

@Strain 100 %
>= 1450 psi

@Strain 100 %
ISO 37
>= 23.0 MPa

@Strain 300 %
>= 3340 psi

@Strain 300 %
ISO 37
Elongation at Yield >= 420 %
>= 420 %
ISO 37
Tear Strength >= 120 kN/m
>= 685 pli
ISO 34
K Factor (Wear Factor) <= 60
<= 60
[mm<sup>3</sup>]; ISO 4649
Compression Set <= 40 %

@Temperature 70.0 °C
<= 40 %

@Temperature 158 °F
ISO 815