Physical Properties Metric English Comments
Density 1.11 - 1.12 g/cc
0.0401 - 0.0405 lb/in³
Average value: 1.12 g/cc Grade Count:5
Overview of materials for Nylon 6/69
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6/69". Each property range of values reported is minimum and maximum values of appropriate MatWeb ..
Density 1.12 - 1.12 g/cc

@Temperature >=250 °C
0.0405 - 0.0405 lb/in³

@Temperature >=482 °F
Average value: 1.12 g/cc Grade Count:1
Overview of materials for Nylon 612, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of ..
Density 1.10 - 1.12 g/cc
0.0397 - 0.0405 lb/in³
ASTM D1505
Specialty Coating Systems Parylene N Poly (P-Xylylene) Coating
Parylene N, poly(para-xylylene), is a completely linear, highly crystalline material. Parylene N is a primary dielectric, exhibiting a very low dissipation factor, high dielectric strength, and a lo..
Density 1.08 - 1.12 g/cc
0.0390 - 0.0405 lb/in³
ISO 1183
Austin Novel Materials Texalan® 265A Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech
Density 1.08 - 1.12 g/cc
0.0390 - 0.0405 lb/in³
ISO 1183
Austin Novel Materials Texalan® 365A Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech
Density 1.08 - 1.12 g/cc
0.0390 - 0.0405 lb/in³
ISO 1183
Austin Novel Materials Texalan® 465A Polyester-based TPU
Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech
Density 1.08 - 1.12 g/cc
0.0390 - 0.0405 lb/in³
ISO 1183
Austin Novel Materials Texalan® 582A Polyether-based TPU
Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech
Density 1.08 - 1.12 g/cc
0.0390 - 0.0405 lb/in³
ISO 1183
Austin Novel Materials Texalan® 665A Polyester and Polyether based TPU
Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech
Density 1.09 - 1.12 g/cc
0.0394 - 0.0405 lb/in³
Average value: 1.11 g/cc Grade Count:11
Overview of materials for Ethyl Cellulose, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Ethyl Cellulose, Molded". Each property range of values reported is minimum and maximum values of approp..
Density 1.08 - 1.12 g/cc
0.0390 - 0.0405 lb/in³
ISO 1183
Austin Novel Materials Texalan® 782A PCL TPU
Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech