SABIC Innovative Plastics NORYL PKN4752 PPE+PS (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL PKN4752 PPE+PS (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
NORYL PKN4752 is a translucent, high heat PPO+PS extrusion grade for dilution with polystyrene resin. It is suitable for (microwavable) food packaging and is compliant with US and European food contact regulations.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 86.0 MPa
12500 psi
50 mm/min; ISO 527
Elongation at Break 6.0 %
6.0 %
50 mm/min; ISO 527
Tensile Modulus 3.10 GPa
450 ksi
1 mm/min; ISO 527
Flexural Yield Strength 130 MPa
18900 psi
2 mm/min; ISO 178
Flexural Modulus 2.95 GPa
428 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
80*10*4; ISO 180/1A
3.00 kJ/m²

@Temperature -30.0 °C
1.43 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
0.200 J/cm²

@Temperature -30.0 °C
0.952 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 163 °C
325 °F
Edgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 147 °C
297 °F
Edgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 174 °C
345 °F
Rate A/50; ISO 306