Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Tipco Tipcolene® NPI 200 IN - 25% Talc/Mineral Reinforced Polypropylene Copolymer with Very High Flow, Stiffness & Impact Strength

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Tipco Industries Ltd., India
Trade Name Tipcolene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tipco Tipcolene® NPI 200 IN - 25% Talc/Mineral Reinforced Polypropylene Copolymer with Very High Flow, Stiffness & Impact Strength.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
20% Mineral Reinforced, Very High Stiffness & Very High Impact PP CopolymerApplications: Automotive DashboardsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0125 cm/cm
0.0125 in/in
ASTM D955
Melt Flow 15 g/10 min
15 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 75
75
Tensile Strength, Yield 19.5 MPa
2830 psi
ASTM D638
Elongation at Break >= 90 %
>= 90 %
ASTM D638
Flexural Yield Strength 35.0 MPa
5080 psi
ASTM D790
Flexural Modulus 2.70 GPa
392 ksi
ASTM D790
Izod Impact, Notched (ISO) 40.0 kJ/m²
19.0 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 130 °C
266 °F
ASTM D648