Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Elvax® 3200-2 Ethylene-Vinyl Acetate Copolymer Resin for Extrusion Coating

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade
Manufacturer DuPont Packaging and Industrial Polymers
Trade Name Elvax®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Elvax® 3200-2 Ethylene-Vinyl Acetate Copolymer Resin for Extrusion Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
22.5 wt% Vinyl Acetate.Elvax® 3200-2 is an extrudable, wax-modified, ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.Additives: Antioxidant.Applications: Elvax® 3200-2 is designed to provide a low temperature peelable heat seal to itself or many other materials commonly used in flexible packaging applications. The melt properties of this resin allow it to be processed on extrusion coating equipment over a wide range of line speeds and coating thicknesses. It can also be coextrusion coated with a variety of other polymers. Elvax® 200-2 is typically used as a lidding sealant for a variety of formed containers, in replacement of solvent applied heat seal lacquers. It will provide a good seal against HDPE film and sheet, polypropylene film, PVDC, rigid vinyl, rigid and foamed polystyrene, and nitrocellulose coatings.Information provided by DuPont Packaging Polymers.
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ASTM D792
Melt Flow 32 g/10 min
32 g/10 min
Condition not noted.; ASTM D1238
Mechanical Properties Metric English Comments
Coefficient of Friction 0.48
0.48
coating/metal; ASTM D1894
0.95
0.95
coating/coating; ASTM D1894
Thermal Properties Metric English Comments
Melting Point 55.0 °C
131 °F
Freezing Point via DSC/ASTM D3418
71.0 °C
160 °F
Upon Melting via DSC/ASTM D3418
Vicat Softening Point 55.0 °C
131 °F
ASTM D1525
Processing Properties Metric English Comments
Melt Temperature 200 - 232 °C
392 - 450 °F