Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.18 - 1.25 g/cc | 0.0426 - 0.0452 lb/in³ | |
Reliance Industries METABOLIX PHB Information provided by Reliance Industries |
|||
Density | 1.15 - 1.25 g/cc | 0.0415 - 0.0452 lb/in³ | Apparent |
Gouda Vuurvast FI 65-12 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |
|||
Density | 1.14 - 1.25 g/cc | 0.0412 - 0.0452 lb/in³ | 253 Resin |
Lord Adhesives Versilok® 253 / 254 Acrylic Adhesive LORD Versilok® 253/254 adhesive is a two-component, epoxy-modified acrylic adhesive used to bond a variety of automotive sheet metals, including hot-dip galvanized, electro-galvanized, bare alum.. |
|||
Density | 1.20 - 1.25 g/cc | 0.0434 - 0.0452 lb/in³ | |
Sibur 1045-12 Compound 948 Polyvinyl Chloride (PVC) Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a p.. |
|||
Density | 1.18 - 1.25 g/cc | 0.0426 - 0.0452 lb/in³ | |
Sibur O-55 Compound 1182 Polyvinyl Chloride (PVC) Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a p.. |
|||
Density | 1.15 - 1.25 g/cc | 0.0415 - 0.0452 lb/in³ | ASTM D792 |
Sumitomo Bakelite North America EM 7302XLD Long Glass Fiber Reinforced Epoxy EM 7302XLD is a long fiberglass reinforced epoxy molding compound with a low density inert filler. This compound is designed for applications where moderate strength and weight savings are desirable.. |
|||
Density | 1.15 - 1.25 g/cc | 0.0415 - 0.0452 lb/in³ | FTTC 2443 |
Formosa Plastics 12.5% Sodium Hypochlorite Information provided by Formosa Plastics Corporation, USA |
|||
Density | 1.15 - 1.25 g/cc | 0.0415 - 0.0452 lb/in³ | |
Dow BETAMATE™ 7200 Polyurethane Prepolymer BETAMATE™ 7200 is a one component moisture curing polyurethane seam sealant with permanent elasticity and good adhesion to different substrates. It is an excellent seam sealer for body repair. It.. |
|||
Density | 1.15 - 1.25 g/cc | 0.0415 - 0.0452 lb/in³ | |
Dow BETAMATE™ 7205 Polyurethane Prepolymer BETAMATE™ 7205 is a one component moisture curing polyurethane seam sealant with permanent elasticity and good adhesion to different substrates. It is an excellent seam sealer for body repair. It.. |
|||
Density | 1.21 - 1.25 g/cc | 0.0437 - 0.0452 lb/in³ | ISO R 1183 |
Fainplast Compounds FAINGUM 7010 Flexible PVC, Injection Molding for Footwear Soles with rubber |
|||
Density | 1.21 - 1.25 g/cc | 0.0437 - 0.0452 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 7004 Flexible PVC, Injection Molding for Footwear Sandals for armed force, antifungus |
|||
Density | 1.21 - 1.25 g/cc | 0.0437 - 0.0452 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 82/SN Flexible PVC, Injection Molding for Transparent Technical Items Technical items high transparency |
|||
Density | 1.21 - 1.25 g/cc | 0.0437 - 0.0452 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 87/BT Flexible PVC, Injection Molding for Transparent Technical Items Technical items low temperatures |
|||
Density | 1.21 - 1.25 g/cc | 0.0437 - 0.0452 lb/in³ | ISO R 1183 |
Fainplast Compounds GSO 65/33 Flexible PVC, Injection Molding for Footwear Soles, opaque surface |
|||
Density | 1.20 - 1.25 g/cc | 0.0434 - 0.0452 lb/in³ | ASTM D792, ISO 1183 |
EPICHEM Epiryl G2 PPO 20GF Polyphenylene oxide, 20% Glass Fiber Characteristics: 20% glass fibre filled |
|||
Density | 1.21 - 1.25 g/cc | 0.0437 - 0.0452 lb/in³ | ISO R 1184 |
Fainplast Compounds MPH 75/H Medical Flexible PVC, Extrusion Technical tubes no DOP |
|||
Density | 1.21 - 1.25 g/cc | 0.0437 - 0.0452 lb/in³ | ISO R 1184 |
Fainplast Compounds MPH 78 Medical Flexible PVC, Extrusion Tubolar apparatus |
|||
Density | 1.21 - 1.25 g/cc | 0.0437 - 0.0452 lb/in³ | ISO R 1184 |
Fainplast Compounds MPH 83/T Medical Flexible PVC, Extrusion Technical tubes no DOP |
|||
Density | 1.21 - 1.25 g/cc | 0.0437 - 0.0452 lb/in³ | ISO R 1183 |
Fainplast Compounds PH 75/C Flexible PVC, Transparent Extrusion Profiles, UL 94 Class V1 |
|||
Density | 1.21 - 1.25 g/cc | 0.0437 - 0.0452 lb/in³ | ISO R 1183 |
Fainplast Compounds PHT 0144 Flexible PVC, Transparent Extrusion Profiles high temperatures |
|||
Density | 1.21 - 1.25 g/cc | 0.0437 - 0.0452 lb/in³ | ISO R 1184 |
Fainplast Compounds KLT 93 Flexible PVC, Insulation Transparent Cables Lead Free Transparent cables (105°C) |
|||
Density | 1.21 - 1.25 g/cc | 0.0437 - 0.0452 lb/in³ | ISO R 1183 |
Fainplast Compounds MGS 75 Medical Flexible PVC, Injection Molding Connectors and special components |
|||
Density | 1.21 - 1.25 g/cc | 0.0437 - 0.0452 lb/in³ | ISO R 1183 |
Fainplast Compounds MGS 79 Medical Flexible PVC, Injection Molding Connectors and special components |
|||
Density | 1.21 - 1.25 g/cc | 0.0437 - 0.0452 lb/in³ | ISO R 1183 |
Fainplast Compounds PH 58/AL Flexible PVC, Transparent Extrusion Pipes according to dir. 2002/72/CE |
|||
Density | 1.21 - 1.25 g/cc | 0.0437 - 0.0452 lb/in³ | ISO R 1183 |
Fainplast Compounds PM 64/OP Flexible PVC, Lead Free Gaskets, Opaque surface |
|||
Density | 1.15 - 1.25 g/cc | 0.0415 - 0.0452 lb/in³ | Apparent |
Gouda Vuurvast FI 25-12 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |
|||
Density | 1.15 - 1.25 g/cc | 0.0415 - 0.0452 lb/in³ | Apparent |
Gouda Vuurvast FI 35-12 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |
|||
Density | 1.21 - 1.25 g/cc | 0.0437 - 0.0452 lb/in³ | ISO R 1183 |
Fainplast Compounds PMP 102 Flexible PVC, Extrusion Modified with PU Oil resistant sheath |
|||
Density | 0.950 - 1.25 g/cc | 0.0343 - 0.0452 lb/in³ | Average value: 1.16 g/cc Grade Count:11 |
Overview of materials for Thermoset Polyurethane, Elastomer, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Elastomer, Glass Filled". Each property range of values reported is minimum and .. |