Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Braskem Evateno® HM 2528 EVA Hot Melt Copolymer

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
Manufacturer Braskem
Trade Name Evateno®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem Evateno® HM 2528 EVA Hot Melt Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Evateno® HM 2528 is a copolymer of Ethylene-Vinyl Acetate (EVA) with high vinyl-acetate content, low molecular weight, and good compatibility with other thermoplastic and elastomeric resins, and it can be used in blends with other polyethylenes to improve environmental stress cracking resistance (ESCR), impact resistance, and brittleness at low temperatures. It contains antioxidant additives. Its applications include: hot-melt adhesives, coating, expanded parts, and injection molded and extrusion molded parts where flexibility, resilience, and environmental stress crack resistance (ESCR) are required. Hot-melt adhesives formulation presents excellent compatibility with wax, paraffins, and tackifiers, improving the flexibility and adherence.
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ASTM-D1505 / ASTM-D792
ESCR 100% Igepal® >= 300 hour

@Thickness 2.00 mm,
Temperature 50.0 °C
>= 300 hour

@Thickness 0.0787 in,
Temperature 122 °F
0.3 mm notched-plaques; ASTM-D1693
Vinyl Acetate Content 28 %
28 %
Melt Flow 25 g/10 min

@Load 2.16 kg,
Temperature 190 °C
25 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 79
79
ASTM-D2240
Hardness, Shore D 23
23
ASTM-D2240
Thermal Properties Metric English Comments
Melting Point 75.0 °C
167 °F
ASTM-D3418
Vicat Softening Point 46.0 °C

@Load 1.02 kg
115 °F

@Load 2.25 lb
ASTM-D1525
Users viewing this material also viewed the following: