Indium Corp. Indalloy 101 Bismuth-Lead-Tin Solder Alloy

Category Metal , Nonferrous Metal , Lead Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 101 Bismuth-Lead-Tin Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 9.47 g/cc
0.342 lb/in³
Thermal Properties Metric English Comments
Melting Point 130 - 173 °C
266 - 343 °F
Solidus 130 °C
266 °F
Liquidus 173 °C
343 °F
Component Elements Properties Metric English Comments
Bismuth, Bi 20 %
20 %
Lead, Pb 50 %
50 %
Tin, Sn 30 %
30 %