Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 9.47 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 9.47 g/cc
0.342 lb/in³
Indium Corp. Indalloy 140 Bismuth Solder Alloy
Information Provided by Indium Corporation
Density 9.47 g/cc
0.342 lb/in³
Indium Corp. Indalloy 101 Bismuth-Lead-Tin Solder Alloy
Information Provided by Indium Corporation
Copyright © lookpolymers.com All Rights Reserved