Indium Corp. Indalloy 47 Bismuth-Lead-Tin Solder Alloy

Category Metal , Nonferrous Metal , Bismuth Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 47 Bismuth-Lead-Tin Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 9.48 g/cc
0.342 lb/in³
Thermal Properties Metric English Comments
Melting Point 70.0 - 105 °C
158 - 221 °F
Solidus 70.0 °C
158 °F
Liquidus 105 °C
221 °F
Component Elements Properties Metric English Comments
Bismuth, Bi 35.3 %
35.3 %
Cadmium, Cd 9.5 %
9.5 %
Lead, Pb 35.1 %
35.1 %
Tin, Sn 20.1 %
20.1 %