Material Notes:
CPM S90V is a unique tool steel made by the Crucible Particle Metallurgy process. It is a martensitic stainless steel with a high volume of vanadium carbides for exceptionally good wear resistance. S90V offers substantial improvements in wear resistance over 440C and D2, and other high chromium tool steels, with corrosion resistance equal to or better than 440C. Its high vanadium content favors the formation of hard vanadium carbides instead of chromium carbides for wear resistance, leaving sufficient chromium in the matrix to provide good corrosion resistance.The wear and corrosion resistance of S90V make it an excellent candidate to replace 440C, where increased wear is a primary concern. It can replace D2 or other tool steels in applications where improved corrosion resistance is also of benefit.The CPM process results in a finer, more uniform carbide distribution imparting improved toughness and grindability to high alloy steels. The CPM process also allows the design of more highly alloyed grades which cannot be produced by conventional steelmaking.Information provided by Crucible Specialty Metals.
Physical Properties Metric English Comments
Density 7.40 g/cc
0.267 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 277
277
Annealed
Hardness, Rockwell C 56 - 59
56 - 59
Modulus of Elasticity 215 GPa
31200 ksi
Charpy Impact 27.12 J
20.00 ft-lb
Thermal Properties Metric English Comments
CTE, linear 11.0 µm/m-°C

@Temperature 20.0 - 200 °C
6.11 µin/in-°F

@Temperature 68.0 - 392 °F
Thermal Conductivity 17.3 W/m-K

@Temperature 65.0 °C
120 BTU-in/hr-ft²-°F

@Temperature 149 °F
Shrinkage -0.0500 - -0.0300 %
-0.0500 - -0.0300 %
Component Elements Properties Metric English Comments
Carbon, C 2.3 %
2.3 %
Chromium, Cr 14 %
14 %
Iron, Fe 73.7 %
73.7 %
As Remainder
Tungsten, W 1.0 %
1.0 %
Vanadium, V 9.0 %
9.0 %
Descriptive Properties Value Comments
Corrosion Rate; mm/y 102 to 117
Dilute Aqua-Regia
9 to 17
10% Boiling Acetic