American Elements Europium Oxide Nanopwder

Category Ceramic , Oxide
Manufacturer American Elements
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF American Elements Europium Oxide Nanopwder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General DescriptionEU-MITE powders and dispersions are inorganic europium-oxide nanoparticles. EU-MITE-A products are uncoated and hydrophilic. EU-MITE-O products are coated with an organic silane (1-4%) and are hydrophobic. Particles are available in the size range of 10-200 nm.
Physical Properties Metric English Comments
Density 7.40 g/cc
0.267 lb/in³
Molecular Weight 351.92 g/mol
351.92 g/mol
Thermal Properties Metric English Comments
Melting Point 2350 °C
4260 °F
Descriptive Properties Value Comments
Appearance White
Solubility Insoluble in water, moderately soluble in strong mineral acids
Stability Slightly hygroscopic