Material Notes:
High temperature electrical solderInformation Provided by Indium Corporation
Physical Properties Metric English Comments
Density 7.39 g/cc
0.267 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 13.7
13.7
Tensile Strength at Break 55.2 MPa
8000 psi
Elongation at Break 30 %
30 %
Shear Strength 24.4 MPa
3540 psi
Thermal Properties Metric English Comments
CTE, linear 23.0 µm/m-°C

@Temperature 20.0 °C
12.8 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 0.230 J/g-°C
0.0550 BTU/lb-°F
Solid
Melting Point 221 - 240 °C
430 - 464 °F
Solidus 221 °C
430 °F
Liquidus 240 °C
464 °F
Component Elements Properties Metric English Comments
Silver, Ag 5.0 %
5.0 %
Tin, Sn 95 %
95 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000137 ohm-cm
0.0000137 ohm-cm