Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.81 g/cc | 0.0654 lb/in³ | |
Pyrotek TS-110 Thermoset Electrical Insulation Product (Nema Grade: G-10) Glass reinforcement, Epoxy Resin, Natural Color. High flexural, impact and bond strength at room temperature.Information provided by Pyrotek. |
|||
Density | 1.81 g/cc | 0.0654 lb/in³ | ISO 1183 |
Hexion Bakelite™ MP 4165 Melamine Phenolic Resin, Copper Adhesive, Low Shrinkage, High Mechanical Strength
(d Melamine/phenolic molding compound, inorganically filled, glass fiber reinforced, good temperature stability, high level of mechanical properties, copper adhesive, flammability UL 94/V-0/1.6 mm (not.. |
|||
Density | 1.81 g/cc | 0.0654 lb/in³ | ISO 1183 |
Menzolit Menzolit® BMC 2900 Unsaturated Polyester UP BMC 2900 is a specially designed BMC to meet the EC Safety Signs Directive (92/58/EEC) on the provision and use of safety signs at work. In areas where it is not possible to include the use of illu.. |
|||
Density | 1.81 g/cc | 0.0654 lb/in³ | ISO R 1183 |
Multibase Multibatch® MP 52214 Injection Molding HPP. 75% CaCO3, 10%TiO2FilledFine Particle Size.Information provided by Multibase |
|||
Density | 1.81 g/cc | 0.0654 lb/in³ | Real Density |
SGL Carbon Group CF 5250 Carbon Filler Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Density | 1.81 g/cc | 0.0654 lb/in³ | |
SGL Carbon Group EK 2241 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Density | 1.81 g/cc | 0.0654 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Tecnoflon® FOR TF 636 Fluoroelastomer TECNOFLON® FOR TF 636 is a medium-low viscosity cure incorporated fluoroelastomer terpolymer designed to provide improved low temperature characteristics. Tecnoflon® FOR TF 636 exhibits the sa.. |
|||
Density | 1.81 g/cc | 0.0654 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® 7062 PBT+PET (Europe-Africa-Middle East) Valox 7062 is Mineral filled PBT injection molding grade. |
|||
Density | 1.81 g/cc | 0.0654 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® 7062HP PBT ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Density | 1.81 g/cc | 0.0654 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® 7062HP PBT (Asia Pacific) ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Density | 1.81 g/cc | 0.0654 lb/in³ | |
Zoltek Panex 35® 50k Continuous Tow Commercial Carbon Fiber for Industrial Applications Commercial Carbon Fiber for Industrial Applications |
|||
Density | 1.81 g/cc | 0.0654 lb/in³ | |
Zoltek Panex 35® Tow Weave Carbon Fiber Fabrics Tow Weave Carbon Fiber Fabrics |
|||
Density | 1.81 g/cc | 0.0654 lb/in³ | |
Cytec Thornel® T-40 12K Carbon Fiber, Polyacrylonitrile (PAN) Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t.. |
|||
Density | 1.81 g/cc | 0.0654 lb/in³ | |
Cytec Thornel® T-50 6K Carbon Fiber, Polyacrylonitrile (PAN) Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t.. |
|||
Density | 1.81 g/cc | 0.0654 lb/in³ | ISO 1183 |
Barlog Plastics KEBATER BM240 PBT, 40% mineral reinforced, food grade (PBT+X)-MD40Information provided by BARLOG plastics GmbH. |
|||
Density | 1.81 g/cc | 0.0654 lb/in³ | |
A. Schulman ComAlloy Hiloy® 422 Heavy Mineral Reinforced, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.40% Heavy Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Density | 1.81 g/cc @Temperature -70.0 °C |
0.0654 lb/in³ @Temperature -94.0 °F |
|
3M Novec™ 7500 Engineered Fluid 3M™ Novec™ 7500 is a non-flammable fluid with a very low global warming potential (GWP.) Its' excellent inerting and dielectric properties make it a viable replacement for higher GWP fluids such a.. |
|||
Density | 1.81 - 1.85 g/cc | 0.0654 - 0.0668 lb/in³ | ISO R 1183 |
Fainplast Compounds PM 83/M Flexible PVC, Extrusion Covering copper pipes |
|||
Density | 1.81 g/cc | 0.0654 lb/in³ | ASTM D-792 |
Sumitomo Bakelite North America FM 4017F Fiberglass and Mineral Reinforced Phenolic FM 4017F is a fiberglass and mineral reinforced phenolic molding compound, with excellent dimensional stability and good strength at elevated temperatures. Information supplied by Sumitomo Bak North.. |
|||
Density | 1.81 g/cc @Temperature -120 °C |
0.0654 lb/in³ @Temperature -184 °F |
|
3M Novec™ 7000 Engineered Fluid 3M™ Novec™ 7000 Fluid unique properties make it useful as a low temperature, heat transfer fluid for cooling reactors in pharmaceutical & chemical processing. It's also ideal for low temperature a.. |
|||
Density | 1.81 g/cc | 0.0654 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
Arlon R37503G060 0.060" Uncured Fluorosilicone on Release PET Carrier Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured FluorosiliconeCarrier: 0.005" Release PETThis data represents typical values for the production material and should not be used .. |
|||
Density | 1.81 g/cc | 0.0654 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Amodel® AF-1145 V0 Polyphthalamide (PPA) Resin, 45% Glass Reinforced, Dry As Molded
  AMODEL AF-1145 V0 is a 45% glass reinforced, flame retarded polyphthalamide (PPA) which exhibits a high heat distortion temperature, high tensile strength and flexural modulus. The material is rela.. |