Material Notes:
3M™ Novec™ 7500 is a non-flammable fluid with a very low global warming potential (GWP.) Its' excellent inerting and dielectric properties make it a viable replacement for higher GWP fluids such as PFCs and PFPEs in a wide variety of applications.Features and Benefits:Wide range of thermal management applicationsWide liquid rangeNon-flammableNon-conductive Compatible with plasticsLow toxicityLow Global Warming Potential (GWP)Zero ozone depletion potentialVOC-exempt solvent (US EPA)Information provided by 3M
Physical Properties Metric English Comments
Density 1.614 g/cc
0.05831 lb/in³
Liquid
1.40 g/cc

@Temperature 130 °C
0.0506 lb/in³

@Temperature 266 °F
1.60 g/cc

@Temperature 30.0 °C
0.0578 lb/in³

@Temperature 86.0 °F
1.81 g/cc

@Temperature -70.0 °C
0.0654 lb/in³

@Temperature -94.0 °F
Kinematic Viscosity 0.28 cSt

@Temperature 110 °C
0.28 cSt

@Temperature 230 °F
0.50 cSt

@Temperature 50.0 °C
0.50 cSt

@Temperature 122 °F
15 cSt

@Temperature -10.0 °C
15 cSt

@Temperature 14.0 °F
50 cSt

@Temperature -80.0 °C
50 cSt

@Temperature -112 °F
Viscosity Measure 0.77 cSt
0.77 cSt
Molecular Weight 414 g/mol
414 g/mol
Surface Tension 16.2 dynes/cm
16.2 dynes/cm
Thermal Properties Metric English Comments
Heat of Vaporization 88.5 J/g

@Pressure 0.101 MPa
38.1 BTU/lb

@Pressure 14.7 psi
CTE, linear 1290 µm/m-°C
717 µin/in-°F
Specific Heat Capacity 0.980 J/g-°C

@Temperature -70.0 °C
0.234 BTU/lb-°F

@Temperature -94.0 °F
1.06 J/g-°C

@Temperature -20.0 °C
0.253 BTU/lb-°F

@Temperature -4.00 °F
1.14 J/g-°C

@Temperature 30.0 °C
0.272 BTU/lb-°F

@Temperature 86.0 °F
1.21 J/g-°C

@Temperature 80.0 °C
0.289 BTU/lb-°F

@Temperature 176 °F
1.29 J/g-°C

@Temperature 130 °C
0.308 BTU/lb-°F

@Temperature 266 °F
Thermal Conductivity 0.0530 W/m-K

@Temperature 130 °C
0.368 BTU-in/hr-ft²-°F

@Temperature 266 °F
0.0580 W/m-K

@Temperature 80.0 °C
0.403 BTU-in/hr-ft²-°F

@Temperature 176 °F
0.0650 W/m-K

@Temperature 30.0 °C
0.451 BTU-in/hr-ft²-°F

@Temperature 86.0 °F
0.0720 W/m-K

@Temperature -20.0 °C
0.500 BTU-in/hr-ft²-°F

@Temperature -4.00 °F
0.0830 W/m-K

@Temperature -70.0 °C
0.576 BTU-in/hr-ft²-°F

@Temperature -94.0 °F
Boiling Point 128 °C

@Pressure 0.101 MPa
262 °F

@Pressure 14.7 psi
Pour Point -100 °C
-148 °F
Electrical Properties Metric English Comments
Volume Resistivity 2.20e+8 ohm-cm
2.20e+8 ohm-cm
Dielectric Constant 5.8
5.8
Dielectric Strength 1.38 kV/mm
35.0 kV/in
0.1" gap
Chemical Properties Metric English Comments
Critical Pressure 15.5 bar
11600 torr
Critical Temperature 216 °C
421 °F
Descriptive Properties Value Comments
Solubility <3 ppm