Material Notes:
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and good electrical conductivity.Typical Applications: Carbon filler with amorphous structureInformation provided by SGL Carbon Group
Physical Properties Metric English Comments
Bulk Density 0.460 g/cc
0.0166 lb/in³
0.710 g/cc
0.0257 lb/in³
Tap Density
Density 1.81 g/cc
0.0654 lb/in³
Real Density
Particle Size <= 1.0 µm
<= 1.0 µm
10%
<= 8.0 µm
<= 8.0 µm
28%
<= 32 µm
<= 32 µm
60%
<= 64 µm
<= 64 µm
86%
<= 96 µm
<= 96 µm
97%
Specific Surface Area 1.97 m²/g
1.97 m²/g
Blaine
Ash <= 1.0 %
<= 1.0 %
Processing Properties Metric English Comments
Moisture Content <= 1.0 %
<= 1.0 %