Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Tecnoflon® FOR TF 636 Fluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Solvay Specialty Polymers
Trade Name Tecnoflon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Tecnoflon® FOR TF 636 Fluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TECNOFLON® FOR TF 636 is a medium-low viscosity cure incorporated fluoroelastomer terpolymer designed to provide improved low temperature characteristics. Tecnoflon® FOR TF 636 exhibits the same excellent heat and chemical resistance expected from Tecnoflon® copolymers. Tecnoflon ® FOR TF 636 can be used for compression, injection and transfer molding of O-rings, diaphragms, gaskets, seals, molded shapes or other items requiring improved low temperature performance. Tecnoflon ® FOR TF 636 can be combined with the cure system and other typical fluoroelastomer compounding ingredients. Mixing can be accomplished with two roll mills or internal mixers.Features: Good Chemical Resistance; Good Mold Release; High Flow; High Heat Resistance; Low Compression Set; Medium-low Viscosity; TerpolymerUses: Belts/Belt Repair; Blending; Diaphragms; Gaskets; Hose; Profiles; Seals; SheetAdditional Properties: Compound Tested - 6 %; Compound Tested - 3 %; Compound Tested - 30 %; Compound Tested - 100 %; Fluorine Content - Internal Method 66 %; MDR 6 min @ 177°C arc 0.5° - ASTM D6601 3.0 N·m; MDR 6 min @ 177°C arc 0.5° - ASTM D6601 0.16 N·m; MDR 6 min @ 177°C arc 0.5° - ASTM D6601 1.4 min; MDR 6 min @ 177°C arc 0.5° - ASTM D6601 2.1 min; MDR 6 min @ 177°C arc 0.5° - ASTM D6601 1.2 min; Mooney Scorch MS 135°C - ASTM D1646 28 MU; Mooney Scorch MS 135°C - ASTM D1646 24.0 min; ODR 12 min @ 177°C arc 3° - ASTM D2084 15 N·m; ODR 12 min @ 177°C arc 3° - ASTM D2084 1.5 N·m; ODR 12 min @ 177°C arc 3° - ASTM D2084 3.5 min; ODR 12 min @ 177°C arc 3° - ASTM D2084 2.0 min; Solubility - Ketones and esters; Temperature Retraction - ASTM D1329 -19 °C; Temperature Retraction - ASTM D1329 -14 °C; Temperature Retraction - ASTM D1329 -10 °CInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.81 g/cc
0.0654 lb/in³
ASTM D792
Mooney Viscosity 31 - 61

@Temperature 121 °C
31 - 61

@Temperature 250 °F
ML 1+10; ASTM D1646
Mechanical Properties Metric English Comments
Hardness, Shore A 76
76
ASTM D2240
Tensile Strength 18.4 MPa
2670 psi
Die C; ASTM D412
Elongation at Break 170 %
170 %
Die C; ASTM D412
100% Modulus 0.00820 GPa
1.19 ksi
Die C; ASTM D412
Descriptive Properties Value Comments
Availability Europe; North America
Color Off-White
Form Slab
Processing Technique Calendering; Compounding
Compression Molding; Extrusion
Injection Molding; Resin Transfer Molding
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved