Material Notes:
3M™ Novec™ 7000 Fluid unique properties make it useful as a low temperature, heat transfer fluid for cooling reactors in pharmaceutical & chemical processing. It's also ideal for low temperature automated test equipment & wafer processing equipment.Features and Benefits:Low Global Warming PotentialExcellent dielectric propertiesNon-ozone depletingLow toxicityNon-flammableNon-corrosiveGood thermal stabilityUseful at extreme low temperatures (to -120 Degree C)Will not damage electronic equipment in event of leakage or other equipment failureInformation provided by 3M
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
Liquid
1.47 g/cc

@Temperature 0.000 °C
0.0531 lb/in³

@Temperature 32.0 °F
1.70 g/cc

@Temperature -60.0 °C
0.0614 lb/in³

@Temperature -76.0 °F
1.81 g/cc

@Temperature -120 °C
0.0654 lb/in³

@Temperature -184 °F
Kinematic Viscosity 0.32 cSt
0.32 cSt
0.28 cSt

@Temperature 30.0 °C
0.28 cSt

@Temperature 86.0 °F
0.50 cSt

@Temperature -20.0 °C
0.50 cSt

@Temperature -4.00 °F
1.1 cSt

@Temperature -60.0 °C
1.1 cSt

@Temperature -76.0 °F
2.0 cSt

@Temperature -80.0 °C
2.0 cSt

@Temperature -112 °F
4.0 cSt

@Temperature -100 °C
4.0 cSt

@Temperature -148 °F
17 cSt

@Temperature -120 °C
17 cSt

@Temperature -184 °F
Molecular Weight 200 g/mol
200 g/mol
Vapor Pressure 0.646 bar
485 torr
Surface Tension 12.4 dynes/cm
12.4 dynes/cm
Thermal Properties Metric English Comments
Heat of Vaporization 142 J/g
61.1 BTU/lb
Latent
CTE, linear 2190 µm/m-°C
1220 µin/in-°F
Specific Heat Capacity 0.845 J/g-°C

@Temperature -120 °C
0.202 BTU/lb-°F

@Temperature -184 °F
1.04 J/g-°C

@Temperature -60.0 °C
0.249 BTU/lb-°F

@Temperature -76.0 °F
1.24 J/g-°C

@Temperature 3.00 °C
0.296 BTU/lb-°F

@Temperature 37.4 °F
Thermal Conductivity 0.0750 W/m-K
0.521 BTU-in/hr-ft²-°F
0.0720 W/m-K

@Temperature 40.0 °C
0.500 BTU-in/hr-ft²-°F

@Temperature 104 °F
0.0880 W/m-K

@Temperature -40.0 °C
0.611 BTU-in/hr-ft²-°F

@Temperature -40.0 °F
0.100 W/m-K

@Temperature -100 °C
0.694 BTU-in/hr-ft²-°F

@Temperature -148 °F
Boiling Point 34.0 °C

@Pressure 0.101 MPa
93.2 °F

@Pressure 14.7 psi
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+8 ohm-cm
1.00e+8 ohm-cm
Dielectric Constant 7.4
7.4
Dielectric Strength 1.57 kV/mm
40.0 kV/in
Chemical Properties Metric English Comments
Critical Pressure 24.8 bar
18600 torr
Critical Temperature 165 °C
329 °F
Critical Density 0.553 g/cc
0.0200 lb/in³
Descriptive Properties Value Comments
Solubility 0.35
of air in fluid
60 ppmw
of water in fluid
Users viewing this material also viewed the following: