Kazanorgsintez 15313-003 High Pressure Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Film Grade
Manufacturer Kazanorgsintez
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kazanorgsintez 15313-003 High Pressure Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Production Method: HDPE is produced by high pressure ethylene polymerization in tubular reactors. Application: Intended for production of bags, pipes, fittings, articles designed for food contact, toys, films and film articles, shaped-molded parts, etc.Information Provided by Kazanorgsintez
Physical Properties Metric English Comments
Density 0.919 - 0.922 g/cc
0.0332 - 0.0333 lb/in³
Environmental Stress Crack Resistance >= 500 hour
>= 500 hour
Melt Flow 0.30 g/10 min
0.30 g/10 min
±30%
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 9.80 MPa
>= 1420 psi
Elongation at Break >= 600 %
>= 600 %
Tear Strength Test >= 13.7
>= 13.7
MPa
Descriptive Properties Value Comments
Amount of impurities [pcs] 2
Superior Quality
30
2nd Quality
8
Premium Quality
Extractable Substance Weight Content (%) 0.4
Extra Class
0.6
1st and 2nd Class