| Category | Polymer , Thermoplastic , Cyclo Olefin Polymer |
| Manufacturer | Zeon Chemicals |
| Trade Name | Zeonex® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Zeon Chemicals Zeonex® 480R Cyclo-Olefin Polymer.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.01 g/cc | 1.01 g/cc | |
| Water Absorption | <= 0.010 % | <= 0.010 % | |
| Melt Flow | 17 - 25 g/10 min <br>@Load 2.16 kg,<br> Temperature 280 °C |
17 - 25 g/10 min <br>@Load 4.76 lb,<br> Temperature 536 °F |
Z-011A |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 60.001 MPa | 8702.4 psi | |
| Elongation at Yield | 40 % | 40 % | |
| Tensile Modulus | 2.20 GPa | 319 ksi | |
| Flexural Strength | 96.0 MPa | 13900 psi | |
| Flexural Modulus | 2.10 GPa | 305 ksi | |
| Izod Impact, Notched | 0.235 J/cm | 0.441 ft-lb/in |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Glass Transition Temp, Tg | 138 °C | 280 °F |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Refractive Index | 1.525 | 1.525 | |
| Transmission, Visible | 92 % | 92 % |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Colored Pellet Content (Black Spots) (pcs/500g) | 0 |