Videolar 825 E High Impact Polystyrene (HIPS)

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer Videolar
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Videolar 825 E High Impact Polystyrene (HIPS).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Grade designed specially for extrusion and thermoformingCharacteristics make it especially suitable for industrial packaging deep draw thermoforming and custom multilayer sheet extrusionFeatures: Stress crack resistanceGood temperature resistanceApplications: Refrigerator and packagingSheet, film and profile extrusionInformation provided by Dax Resinas
Physical Properties Metric English Comments
Bulk Density 0.650 g/cc
0.0235 lb/in³
ISO 060
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
Melt Flow 3.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 23.0 MPa
3340 psi
ASTM D638
Elongation at Yield 55 %
55 %
ASTM D638
Tensile Modulus 1.93 GPa
280 ksi
ASTM D638
Flexural Strength 47.0 MPa
6820 psi
ASTM D790
Flexural Modulus 2.14 GPa
310 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
Falling Dart Impact 14.0 J
10.3 ft-lb
ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 92.0 °C
198 °F
@ 264 psi; ASTM D648
Vicat Softening Point 99.0 °C
210 °F
ASTM D1525
Flammability, UL94 HB
HB