Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Entec Hylex® P1017L2 HB Polycarbonate

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Molded
Manufacturer Entec Engineered Resins
Trade Name Hylex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Entec Hylex® P1017L2 HB Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Available in North America Additive: Mold Release Features: Good Mold Release and High Flow RoHS Compliant Form: Pellets Appearance: Blue Information provided by Entec
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Water Absorption 0.15 %

@Time 86400 sec
0.15 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Melt Flow 17 g/10 min

@Load 1.20 kg,
Temperature 300 °C
17 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 70
70
ASTM D785
Tensile Strength at Break 68.9 MPa
10000 psi
ASTM D638
Elongation at Break 130 %
130 %
ASTM D638
Flexural Strength 95.8 MPa
13900 psi
ASTM D790
Flexural Modulus 2.34 GPa
340 ksi
ASTM D790
Izod Impact, Notched 6.94 J/cm

@Thickness 3.17 mm
13.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 138 °C
280 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 129 °C
265 °F
Unannealed; ASTM D648
Vicat Softening Point 154 °C
310 °F
ASTM D1525
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Optical Properties Metric English Comments
Refractive Index 1.586
1.586
ASTM D542
Haze 1.0 %

@Thickness 3.17 mm
1.0 %

@Thickness 0.125 in
ASTM D1003
Transmission, Visible 88 %

@Thickness 3.17 mm
88 %

@Thickness 0.125 in
ASTM D1003
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+17 ohm-cm
1.00e+17 ohm-cm
ASTM D257
Dielectric Strength 15.0 kV/mm

@Thickness 3.17 mm
380 kV/in

@Thickness 0.125 in
In air; ASTM D149