| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.23 g/cc | 1.23 g/cc | ASTM D792 |
|
PolyOne LubriOne™ PC-000/05T-2S Polycarbonate (PC)
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
|
|||
| Specific Gravity | 1.23 g/cc | 1.23 g/cc | ASTM D792 |
|
PolyOne Maxxam™ XN-418.G001-1000 Polypropylene Copolymer (PP Copolymer)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
|
|||
| Specific Gravity | 1.23 g/cc | 1.23 g/cc | ASTM D-792 |
|
PlastiComp Complet® LCF50 - PP Homopolymer Polypropylene, 50% Long Carbon Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 50% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
|
|||
| Specific Gravity | 1.23 g/cc | 1.23 g/cc | ASTM D792 |
|
Polymer Resources PPX-MF-FR3 Modified-PPO, V-0 Flame Retardant, Mineral Reinforced
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 230F HDT, Mineral ReinforcedFeatures: • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mecha..
|
|||
| Specific Gravity | 1.23 g/cc | 1.23 g/cc | ASTM D792 |
|
Samyang Triloy® 410 PC/PET alloy
(discontinued **)
Characteristics:Impact resistantHeat resistantDimensional stabilityProcessabilityGood flowApplications:O/A partRear view mirror housingRice cooker baseAll information provided by Samyang
|
|||
| Specific Gravity | 1.23 g/cc | 1.23 g/cc | ASTM D792 |
|
Polymer Resources ABS-G25 ABS, 25% Glass Reinforced
Acrylonitrile Butadiene Styrene, 25% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information..
|
|||
| Specific Gravity | 1.23 g/cc | 1.23 g/cc | ASTM D792 |
|
PolyOne Geon™ Vinyl Flexible R4510H Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
|
|||
| Specific Gravity | 1.23 g/cc | 1.23 g/cc | |
|
Sylvin Technologies 8915-65 Natural PVC Extrusion Compound
Information provided by Sylvin Technologies Inc.
|
|||
| Specific Gravity | 1.23 g/cc | 1.23 g/cc | 23°C; ASTM D792 |
|
Teknor Apex APEX® 3300-85 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, RadiationUses-Automotive Applications, Food Service Applications, General Purpose, Med..
|
|||
| Specific Gravity | 1.23 g/cc | 1.23 g/cc | ASTM D792 |
|
Teknor Apex APEX® 3600-85NT Polyvinyl Chloride, Flexible
Uses: Medical/Healthcare Applications Agency Ratings: NSF 61 Forms: Pellets Additional Information: First Generation SeriesInformation Provided by Teknor Apex
|
|||
| Specific Gravity | 1.23 g/cc | 1.23 g/cc | ASTM D792 |
|
Teknor Apex APEX® 3800-80 Polyvinyl Chloride, Flexible
Features: DEHP Plasticizer; Ethylene Oxide Sterilizable; High Heat Resistance Uses: Medical/Healthcare Applications Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor ..
|
|||
| Specific Gravity | 1.23 g/cc | 1.23 g/cc | ASTM D792 |
|
Teknor Apex APEX® 6500-80 Polyvinyl Chloride, Flexible
Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde..
|
|||
| Specific Gravity | 1.23 g/cc | 1.23 g/cc | 23°C; ASTM D792 |
|
Teknor Apex APEX® 94-A0098C-80 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-General Purpose Uses-General PurposeAppearance-ClearForms-PelletsProcessing Method-Injection Molding..
|
|||
| Specific Gravity | 1.23 g/cc | 1.23 g/cc | 23°C; ASTM D792 |
|
Teknor Apex APEX® 2080-H Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-ClearForms-PelletsProcessing Method-Extrusi..
|
|||
| Specific Gravity | 1.23 g/cc | 1.23 g/cc | ASTM D792 |
|
Teknor Apex APEX® 80-C131E-NT Polyvinyl Chloride, Flexible
Notes: RoHS Compliant Forms: PelletsInformation Provided by Teknor Apex
|
|||
| Specific Gravity | 1.23 g/cc | 1.23 g/cc | ASTM D792 |
|
Lubrizol Estane® 58246 Thermoplastic Polyurethane
Features: High stiffness grade with excellent chemical and oil resistance.Uses: Flat Die/Cast Film Extrusion and Injection Molding.Available in Americas, Europe, Middle East, Africa, India and AsiaI..
|
|||
| Specific Gravity | 1.23 g/cc | 1.23 g/cc | ASTM D792 |
|
Eastman Eastar MN004 Copolyester
Eastar Copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. Eastar MN004 contains a mold release.Appl..
|
|||
| Specific Gravity | 1.23 g/cc | 1.23 g/cc | Polymer |
|
DuPont Performance Polymers Neoprene 842A Polychloroprene
DuPont™ Neoprene 842A liquid dispersion contains a medium modulus polychloroprene homopolymer made in an anionic colloidal system. Main Feature - This liquid dispersion gives medium strength cured ..
|
|||
| Specific Gravity | 1.23 g/cc | 1.23 g/cc | ASTM D792 |
|
Clariant Renol 66G15BL-195 Blue Nylon 66, 15% Glass Fiber Reinforced
Data provided by Clariant Masterbatches
|
|||
| Specific Gravity | 1.23 g/cc | 1.23 g/cc | ASTM D792 |
|
Colorite Polymers 92-605 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
|
|||
| Specific Gravity | 1.23 g/cc | 1.23 g/cc | ISO 1183 |
|
Ascend Performance Materials Vydyne® R513H Nylon 66, 13% Glass Filled, Conditioned (2.5% Moisture)
Vydyne® R513H is general-purpose, 13% glass-reinforced, heat stabilized PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow, and mold ..
|
|||
| Specific Gravity | 1.23 g/cc | 1.23 g/cc | ASTM D792 |
|
Asahi Kasei Thermylene® P7-40FG-0790 40% Glass Fiber Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
|
|||
| Specific Gravity | 1.23 g/cc | 1.23 g/cc | ASTM D792 |
|
Colorite Polymers 7866 Non-Phthalate 66 Series Vinyl Compound
Description: The Colorite 66 series is a family of non-toxic PVC compounds developed specifically for those medical device, food, and infant care items for which the use of a citrate* based non-phth..
|
|||
| Specific Gravity | 1.23 g/cc | 1.23 g/cc | ASTM D792 |
|
Teknor Apex Chemlon® 214 GH Nylon 6, 14% Short Glass Fiber
Features: Good Creep Resistance; Good Dimensional Stability; Good Processability; Good Toughness; Heat Stabilized; High Strength Processing Method: Injection Molding Forms: Pellets Additive: Heat S..
|
|||
| Specific Gravity | 1.23 g/cc | 1.23 g/cc | ASTM D792 |
|
Chase Plastics CP Pryme® N213GL (DAM) Nylon 6, 13% Glass Fiber Reinforced, Internally Lubricated
Information provided by Chase Plastics.
|
|||
| Specific Gravity | 1.23 g/cc | 1.23 g/cc | |
|
Sylvin Technologies 5123 PVC Wire/Cable Compound
Information provided by Sylvin Technologies Inc.
|
|||
| Specific Gravity | 1.23 g/cc | 1.23 g/cc | ASTM D792 |
|
A. Schulman POLYFORT™ FPP 1200X High Flow, Calcium Carbonate Fortified Homopolymer Polypropylene
DescriptionPolyfort® FPP 1200X is a high flow 40% calcium carbonate fortified homopolymer polypropylene.Information provided by A. Schulman.
|
|||