| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Arc Resistance | 125 sec | 125 sec | ASTM D495 |
|
Owens Corning Glass Fiber Reinforced Polycarbonate, 10 wt.% glass
Data provided by the manufacturer, Owens Corning.
|
|||
| Arc Resistance | 125 - 135 sec | 125 - 135 sec | ASTM D495 |
|
Raschig Group MELOPLAS® 181 MF
Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. High surface hardness, good electrical properties, good mechanical strength, high UV and heat resistanc..
|
|||
| Arc Resistance | 125 sec | 125 sec | ASTM D495 |
|
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA)
(Unverified Data**)
Amodel A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent creep ..
|
|||
| Arc Resistance | 125 sec | 125 sec | ASTM D495 |
|
Solvay Specialty Polymers Amodel® A-1230 L Polyphthalamide (PPA)
(discontinued **)
Amodel A-1230 L is a 30% mineral filled polyphthalamide (PPA) that offers low warpage and excellent dimensional stability. This resin also has a high deflection temperature, flexural modulus and ten..
|
|||
| Arc Resistance | 125 sec | 125 sec | ASTM D495 |
|
Solvay Specialty Polymers Amodel® A-1240 HS Polyphthalamide (PPA) Resin, 40% Mineral Reinforced, Dry As Molded
&nbs
AMODEL A-1240 polyphthalamide (PPA) resins are 40% mineral filled resins that have high deflection temperature, flexural modulus, and tensile strength. They mold with low warpage, have excellent di..
|
|||
| Arc Resistance | 125 sec | 125 sec | ASTM D495 |
|
Solvay Specialty Polymers Ryton® R-4-230NA Polyphenylene Sulfide Compound
(Unverified Data**)
Natural Color Polyphenylene Sulfide CompoundRyton® R-4-230NA is an advanced 40% fiberglass reinforced polyphenylene sulfide compound which provides reduced flash and improved processability compare..
|
|||
| Arc Resistance | 125 sec | 125 sec | ASTM D495 |
|
Solvay Specialty Polymers Ryton® R-4XT Polyphenylene Sulfide Compound
(Unverified Data**)
Natural Color Polyphenylene Sulfide CompoundRyton® R-4XT is a 40% fiberglass reinforced polyphenylene sulfide compound that takes advantage of state-of-the-art polymerization technology to improve ..
|
|||
| Arc Resistance | 125 sec | 125 sec | ASTM D495 |
|
Solvay Specialty Polymers Ryton® R-4 02XT Polyphenylene Sulfide Compound
(Unverified Data**)
Black Polyphenylene Sulfide CompoundRyton® R-4 02XT is a 40% fiberglass reinforced polyphenylene sulfide compound that takes advantage of state-of-the-art polymerization technology to improve ducti..
|
|||
| Arc Resistance | 125 - 130 sec | 125 - 130 sec | Average value: 128 sec Grade Count:4 |
|
Overview of materials for Nylon 66, Glass/Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of..
|
|||
| Arc Resistance | 125 sec | 125 sec | ASTM D495 |
|
Kolon Kopa® KN173HI Nylon 6 Resin
KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent c..
|
|||
| Arc Resistance | 125 sec | 125 sec | ASTM D495 |
|
Kolon KOPA® KN173HI2 High Impact Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
|
|||
| Arc Resistance | 125 sec | 125 sec | ASTM D495 |
|
Kolon KOPA® KN173HI4 High Impact Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
|
|||
| Arc Resistance | 125 sec | 125 sec | ASTM D495 |
|
Kolon KOPA® KN3322V0Y Flame Retardant Nylon 66
Halogen free, Impact -resistantApplications A variety of connectorsInformation provided by API-Kolon.
|
|||
| Arc Resistance | 125 sec | 125 sec | ASTM D495 |
|
Solvay Specialty Polymers Ryton® R-4 Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4 and R-4-02 40% glass fiber reinforced polyphenylene sulfide compounds provide a good combination of mechanical and electrical properties with outstanding chemical resistance, even at e..
|
|||
| Arc Resistance | 125 sec | 125 sec | ASTM D495 |
|
Solvay Specialty Polymers Ryton® R-4-02 Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4 and R-4-02 40% glass fiber reinforced polyphenylene sulfide compounds provide a good combination of mechanical and electrical properties with outstanding chemical resistance, even at e..
|
|||
| Arc Resistance | 125 sec | 125 sec | ASTM D495 |
|
Solvay Specialty Polymers Ryton® R-4-02XT Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4XT and R-4-02XT 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength with good electrical properties and outstanding chemical resistance, even..
|
|||
| Arc Resistance | 125 sec | 125 sec | ASTM D495 |
|
Solvay Specialty Polymers Ryton® R-4-230BL Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-230NA and R-4-230BL 40% glass fiber reinforced polyphenylene sulfide compounds provide reduced flash and improved processability compared to other polyphenylene sulfide injection moldi..
|
|||
| Arc Resistance | 125 sec | 125 sec | |
|
Cosmic Plastics 306 Orlon Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
|
|||
| Arc Resistance | 125 sec | 125 sec | Absolute Drying; ASTM-D495 |
|
Toyobo GLAMIDE® T-803 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
|
|||
| Arc Resistance | 125 sec | 125 sec | ASTM D495 |
|
Plenco 2300 Phenolic, Granular, Transfer Molded
PLENCO 02300 is a general purpose organic filled molding compound formulated to offer excellent processability while maintaining mechanical strength values. UL recognized under component file E40654..
|
|||
| Arc Resistance | 125 sec | 125 sec | Absolute Drying; ASTM-D495 |
|
Toyobo GLAMIDE® T-802 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
|
|||
| Arc Resistance | 125 sec | 125 sec | IPC TM-650 2.5.1 |
|
Arlon 38N High Performance Polyimide Low-Flow
38N is an improved polyimide low-flow prepreg suitable for bonding multilayer polyimide rigid-flex, attaching heat sinks to polyimide MLBs, or other applications where minimal and uniform resin flow..
|
|||
| Arc Resistance | 125 sec | 125 sec | ASTM D495 |
|
Solvay Specialty Polymers Amodel® A-1240 L Polyphthalamide (PPA)
(discontinued **)
Amodel A-1240 L is a 40% mineral filled polyphthalamide (PPA) that offers low warpage and excellent dimensional stability. This resin also has a high deflection temperature, flexural modulus and ten..
|
|||
| Arc Resistance | 125 sec | 125 sec | ASTM D495 |
|
Owens Corning Glass Fiber Reinforced Polyphenylene Sulfide, 40 wt.% glass
Polyphenylene Sulfide provides excellent resistance to organic solvents (below 375°F). It is unaffected by strong alkalis or aqueous organic salt solutions. Data provided by the manufacturer, Owen..
|
|||
| Arc Resistance | 125 sec | 125 sec | ASTM D495 |
|
Solvay Specialty Polymers Ryton® R-4-220NA Polyphenylene Sulfide Compound
(Unverified Data**)
Natural Color Polyphenylene Sulfide CompoundRyton® R-4-220NA is an advanced 40% fiberglass reinforced polyphenylene sulfide compound formulated for enhanced hydrolytic stability in applications re..
|
|||
| Arc Resistance | 125 - 130 sec | 125 - 130 sec | ASTM D495 |
|
Hexion Bakelite™ PF 2560 Phenolic Formaldehyde Resin, High Surface Quality, For Electrostatic Coating, UL Listed
&n
Phenolic molding compound, inorganically/organically filled, average heat resistant, high surface quality, lower water absorption than PF 31, minimal distortion, UL listed molding compound 1.5 mm/V-..
|
|||