Polymer Property : Izod Impact, Notched = 0.960 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.960 J/cm
1.80 ft-lb/in
ASTM D256-93a
Multibase Multi-Pro® 2005 RC I High Impact 20% Glass Polypropylene
Multi-Pro 2005 RC I is a chemically coupled polypropylene compound with increased stiffness, flex strength and excellent impact resistance. This product is geared for top engineering plastics appli..
Izod Impact, Notched 0.960 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
1.80 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded, Across Flow; ASTM D256A
PolyOne Nymax™ 1280 A HS Black 11 A Polyamide 66 (Nylon 66)
The Nymax® 1200 Blend Series of nylon 6/6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materi..
Izod Impact, Notched >= 0.960 J/cm
>= 1.80 ft-lb/in
ASTM D256
NIZHNEKAMSKNEFTEKHIM 825E High Impact Polystyrene
Grade 825E is a high impact polystyrene designed specifically for extrusion and thermoforming. It is used for production of industrial packaging via deep draw thermoforming and custom multilayer sh..
Izod Impact, Notched >= 0.960 J/cm
>= 1.80 ft-lb/in
ASTM D256
NIZHNEKAMSKNEFTEKHIM 825ES High Impact Polystyrene
Grade 825ES is a high impact polystyrene designed for extrusion and hot molding application. It is suited for hot molded deep drawn industrial packages and multilayer shaped sheet production via ex..
Izod Impact, Notched 0.960 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
1.80 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Nymax™ GF 1204 33 MS 2 Grey A Polyamide 66 (Nylon 66)
The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil..
Izod Impact, Notched 0.960 J/cm
1.80 ft-lb/in
ASTM Data
Dow Questra® QA802 High Heat Syndiotactic Polystyrene, 30% Glass Filled  (discontinued **)
QUESTRA® Crystalline Polymers are semi-crystalline engineering thermoplastic resins produced from styrene monomer using a proprietary metallocene catalyst system. These syndiotactic polymers are ve..
Izod Impact, Notched 0.960 J/cm
1.80 ft-lb/in
ASTM D256
Ineos Nova 1552 High Performance Styrenic Enhanced Polystyrene  (discontinued **)
Easy processing, High modulus, Improve stress whitening, Custom colorsApplications: Injection molding, Office furniture, Electronic media, Photographic equipmentPerformance grades of polystyrene are..
Izod Impact, Notched 0.960 J/cm
1.80 ft-lb/in
ASTM D256
Ineos Nova Zyntar® 7001 High Performance Flame Retardant Polystyrene  (discontinued **)
Super high flow, Reduced processing temperatures, Reduced processing time, Improved aesthetics, Custom colorsApplications: Injection molding, Gas-assist injection molding, Hard to fill cavities, suc..
Izod Impact, Notched 0.960 J/cm

@Thickness 3.17 mm
1.80 ft-lb/in

@Thickness 0.125 in
KEP Kepital® FG2025 25% Glass Fiber Reinforced Acetal Copolymer
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Izod Impact, Notched 0.960 J/cm
1.80 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL SE1GFN1 PPE+PS (Asia Pacific)
10% GR. UL94 V-1 rated. Halogen free flame retardant. Typical applications are TV chassis, deflection yokes and connectors.
Izod Impact, Notched 0.960 J/cm

@Temperature -40.0 °C
1.80 ft-lb/in

@Temperature -40.0 °F
ASTM D256
SABIC Innovative Plastics NORYL SE1GFN2 PPE+PS
PPE+PS blend. 20% Glass reinforced. Non-brominated, non-chlorinated FR system. UL94 V1 and 5VA listing. RTI 110/105/110. Dielectric strength. Dimensional stability. Suitable for E/E applications.
Izod Impact, Notched 0.960 J/cm
1.80 ft-lb/in
ASTM D256
Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA), 16% Glass Fiber (Dry)
Amodel® AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s..
Izod Impact, Notched 0.960 J/cm

@Temperature -30.0 °C
1.80 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics ULTEM D9065 PEI (Asia Pacific)
Polyetherimide blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming.
Izod Impact, Notched 0.960 J/cm
1.80 ft-lb/in
ASTM D256
SABIC Innovative Plastics Valox® 508 PBT+PC
30% GR PBT+PC. Excellent mechanical and thermal performance. Non-flame retardant. Reduced warpage characteristics. Applications same as VALOX 420.
Izod Impact, Notched 0.960 J/cm
1.80 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP STAT-KON DX05499 PC (Asia Pacific)
LNP STAT-KON* DX05499 is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive.
Izod Impact, Notched 0.960 J/cm
1.80 ft-lb/in
ASTM D256
SABIC Innovative Plastics Valox® K4560 PBT (Europe-Africa-Middle East)
30% glass reinforced PBT. Impact modified, high flow, hydrolytically stable.
Izod Impact, Notched 0.960 J/cm
1.80 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP DF0049 PC
LNP THERMOCOMP* DF0049 is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Flame Retardant.
Izod Impact, Notched 0.960 J/cm
1.80 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP RF00AH PA 66 (Asia Pacific)
LNP* Thermocomp* RF00AH is a compound based on Nylon 66 resin containing Glass Fiber.
Izod Impact, Notched 0.960 J/cm
1.80 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP LL004 PEEK (Europe-Africa-Middle East)
LNP LUBRICOMP* LL004 is a compound based on Polyetheretherketone resin containing PTFE. Added features of this material include: Internally Lubricated.
Izod Impact, Notched 0.960 J/cm
1.80 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP STAT-LOY PF303 PA 6 (Asia Pacific)
LNP* Stat-loy* PF303 is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Antistat.
Izod Impact, Notched 0.960 J/cm
1.80 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP RC006 PA 66 (Asia Pacific)
LNP* Thermocomp* RC006 is a compound based on Nylon 66 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Izod Impact, Notched 0.960 J/cm
1.80 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS (Europe-Africa-Middle East)
Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en..
Izod Impact, Notched 0.960 J/cm

@Temperature -40.0 °C
1.80 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Eastman Tenite Propionate 383A2R30009 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 9%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr..
Izod Impact, Notched 0.960 J/cm
1.80 ft-lb/in
ASTM D256
Chem Polymer Chemlon 225-15 MG Nylon 6, 25% Mineral/15% Glass Fiber Reinforced
A 25% mineral reinforced, 15% glass fiber reinforced nylon 6 offering excellent rigidity, dimensional stability and warpage control in large area parts.Data provided by the manufacturer, Chem Polyme..
Izod Impact, Notched 0.960 J/cm
1.80 ft-lb/in
ASTM D256
A. Schulman ComAlloy Hiloy® 114 Polypropylene, Glass Reinforced, Chemically Coupled
Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Notched 0.960 J/cm
1.80 ft-lb/in
ASTM D256
A. Schulman ComAlloy Hiloy® 754 Glass Reinforced, Flow Enhanced, PPS Alloy, UL
Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Notched 0.960 J/cm
1.80 ft-lb/in
ASTM D256
A. Schulman ComAlloy Aqualoy® 140 Polypropylene, Glass Reinforced, Chemically Coupled NSF
Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced. In Aqualoy® materials, carefully selected base resins and proprietary additives meld hydrolytic stability an..
Izod Impact, Notched 0.960 J/cm
1.80 ft-lb/in
ASTM D256
A. Schulman ComAlloy Comtuf® 631 Nylon 6/6, Glass Reinforced, Impact Modified
Data provided by the manufacturer, ComAlloy International Company.13% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int..
Izod Impact, Notched 0.960 J/cm

@Temperature -40.0 °C
1.80 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Eastman Tenite Propionate 350E0096914 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 12%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Izod Impact, Notched 0.960 J/cm
1.80 ft-lb/in
Conditioned; ASTM D256
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad temperature..