| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.10 g/cc | 1.10 g/cc | ASTM D792 |
| Water Absorption | 0.070 % @Time 86400 sec |
0.070 % @Time 24.0 hour |
ASTM D570 |
| Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0070 in/in @Thickness 0.126 in |
SABIC Method |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 115 | 115 | ASTM D785 |
| Tensile Strength, Yield | 43.0 MPa | 6240 psi | SABIC - Japan Method |
| Elongation at Break | 55 % | 55 % | SABIC - Japan Method |
| Flexural Strength | 71.0 MPa | 10300 psi | ASTM D790 |
| Flexural Modulus | 2.25 GPa | 326 ksi | ASTM D790 |
| Izod Impact, Notched | 2.54 J/cm | 4.76 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 70.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
38.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
| Deflection Temperature at 0.46 MPa (66 psi) | 100 °C @Thickness 3.20 mm |
212 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
| Flammability, UL94 | V-1 @Thickness 1.50 mm |
V-1 @Thickness 0.0591 in |
UL 94 |
| V-0 @Thickness 6.00 mm |
V-0 @Thickness 0.236 in |
UL 94 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | 1.00e+16 ohm | 1.00e+16 ohm | ASTM D257 |
| Dielectric Constant | 2.65 @Frequency 50.0 - 60.0 Hz |
2.65 @Frequency 50.0 - 60.0 Hz |