Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact Unnotched = 8.57 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 1.80 J/cm²
8.57 ft-lb/in²
DIN 53453
Nilit FRIANYL A63 CU90 Nylon 6.6 for injection molding, 90% copper filled
Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 1.80 J/cm²
8.57 ft-lb/in²
DIN 53453
Nilit FRIANYL B63 CV40 Nylon 6.6 for injection molding, 40% carbon fiber reinforced
Nylon 6.6 for injection molding, good conductive and electrostatic properties.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 1.80 J/cm²

@Temperature -40.0 °C
8.57 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
Nilit RECONYL A SG30 Recycled nylon 6.6 for injection molding, 30% mineral filled
Recycled nylon 6.6 for injection molding (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 1.80 - 6.00 J/cm²

@Temperature -40.0 - -20.0 °C
8.57 - 28.6 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 3.64 J/cm² Grade Count:7
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar..
Charpy Impact Unnotched 1.80 J/cm²
8.57 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 1200-7116 ABS, with carbon fiber
Applications: Office communication.Electrically conductive, suitable for continuous discharging of statically generated electricity.Information provided by Lehmann & Voss & Co.KG
Charpy Impact Unnotched 1.80 J/cm²
8.57 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 80-7388 Polyacetal-copolymer, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit..
Charpy Impact Unnotched 1.80 J/cm²
8.57 ft-lb/in²
ISO 179/1eU
Lucite International Diakon® CLG356 Acrylic Polymer
Information provided by Lucite International
Charpy Impact Unnotched 1.80 J/cm²
8.57 ft-lb/in²
ISO 179/1eU
Lucite International Diakon® MG100 Acrylic Bead Polymer, High Transparency
PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte..
Charpy Impact Unnotched 1.80 J/cm²
8.57 ft-lb/in²
LATI Larton K/20 PPS, 20% Carbon Fiber Reinforced
Polyphenylene Sulfide (PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Charpy Impact Unnotched 1.80 J/cm²
8.57 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 1105-7583 PEEK, with glass fiber and PTFE, improved wear resistance
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Good friction and wear behaviour especially at increased temperatures.Chemical and hydroly..
Charpy Impact Unnotched 1.80 J/cm²
8.57 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 1200-7116-1 ABS, with carbon fiber
Applications: Office communication.Reduced moment of inertia compared with metal parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Strong, stiff ..
Charpy Impact Unnotched 1.80 J/cm²
8.57 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 1200-7899 ABS, with steel fiber
Applications: Office communication.Electrically conductive, suitable for continuous discharging of statically generated electricity.Isotropic shrinkage characteristics.Information provided by Lehman..
Charpy Impact Unnotched 1.80 J/cm²
8.57 ft-lb/in²
flatwise; ISO 179 1fU
Lehmann & Voss LUVOCOM® 1700-1401 PPO, with carbon fiber and glass fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for..
Charpy Impact Unnotched 1.80 J/cm²
8.57 ft-lb/in²
LATI Larton L K/20 L-PPS, 20% Carbon Fiber Reinforced
Linear Polyphenylene Sulfide (L-PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle..
Charpy Impact Unnotched 1.80 J/cm²
8.57 ft-lb/in²
ISO 179/2C
SABIC Innovative Plastics NORYL LTA6020 PPE+PS (Asia Pacific)
Charpy Impact Unnotched 1.80 J/cm²
8.57 ft-lb/in²
ISO 179/2C
SABIC Innovative Plastics NORYL LTA6020 PPE+PS (Europe-Africa-Middle East)
Charpy Impact Unnotched 1.80 J/cm²
8.57 ft-lb/in²
ISO 179
Chi Mei Kibisan® PN-107 L125 SAN
High Clarity
Charpy Impact Unnotched 1.80 - 8.50 J/cm²
8.57 - 40.5 ft-lb/in²
Average value: 4.46 J/cm² Grade Count:77
Overview of materials for Polyetheretherketone, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum..
Charpy Impact Unnotched 1.80 J/cm²

@Temperature -30.0 °C
8.57 ft-lb/in²

@Temperature -22.0 °F
BASF Novolen® 3300 MC Polypropylene
Data was collected by ISO methods and provided by BASF.
Charpy Impact Unnotched 1.80 - 8.20 J/cm²

@Temperature -30.0 - -20.0 °C
8.57 - 39.0 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 5.75 J/cm² Grade Count:14
Overview of materials for Polypropylene, Long Glass Fiber 50%
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Long Glass Fiber 50%". Specific grades with glass content between 45% and 54% are include..
Charpy Impact Unnotched 1.80 - 7.80 J/cm²
8.57 - 37.1 ft-lb/in²
Average value: 4.03 J/cm² Grade Count:4
Overview of materials for Polypropylene, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum ..
Charpy Impact Unnotched >= 1.80 J/cm²
>= 8.57 ft-lb/in²
ISO 179
Bulk Molding Compounds tetra-DUR N 4203 Bulk Molding Compound
Highest dimensional stability under temp. Low profile.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipat..