| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.13 g/cc | 1.13 g/cc | ASTM D792 |
|
SABIC Innovative Plastics Cycoloy® CY200FC PC+ABS
High flow PC+ABS material designed for local Pacific Automotive applications
|
|||
| Specific Gravity | 1.13 g/cc | 1.13 g/cc | ASTM D792 |
|
Honeywell Aegis™ PL75HS Medium Viscosity, Heat Stabilized, Flexible Nylon 6
(discontinued **)
Description: Aegis PL75HS is a medium viscosity, heat stabilized, flexible nylon 6 especially suited to the production of extrusion profiles offering a combination of good flexibility, toughness and..
|
|||
| Specific Gravity | 1.13 g/cc | 1.13 g/cc | ASTM D792 |
|
Honeywell Aegis™ PL220HS High Viscosity, Heat Stabilized, Flexible Nylon 6
(discontinued **)
Description: Aegis PL220HS is a high viscosity, heat stabilized, flexible nylon 6 especially suited to the production of large diameter extrusion or blow molding profiles offering a combination of g..
|
|||
| Specific Gravity | 1.13 g/cc | 1.13 g/cc | ASTM D1505 |
|
Honeywell Aegis™ H205QP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **)
Description: Aegis H205QP is a lubricated high viscosity, N6 film extrusion grade homopolymer for cast or blown film. It conforms to FDA requirements of 21 CFR 177.1500. It possesses the combination..
|
|||
| Specific Gravity | 1.13 g/cc | 1.13 g/cc | ASTM D1505 |
|
Honeywell Aegis™ HCA155MP Nylon 6/6,6 Extrusion Grade Copolymer
(discontinued **)
Description: Aegis HCA115MP is a lubricated and nucleated high viscosity, nylon 6/6,6 extrusion grade copolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21..
|
|||
| Specific Gravity | 1.13 g/cc | 1.13 g/cc | ASTM D1505 |
|
Honeywell Aegisâ„¢ H100ZP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H100ZP is a medium viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500 as well ..
|
|||
| Specific Gravity | 1.13 g/cc | 1.13 g/cc | ASTM D1505 |
|
Honeywell Aegisâ„¢ H73QP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H73QP is a lubricated low viscosity, nylon 6 extrusion grade homopolymer for cast coextrusion. If conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 as well..
|
|||
| Specific Gravity |
1.13
g/cc <br>@Temperature 23.0 °C
|
1.13
g/cc <br>@Temperature 73.4 °F
|
ASTM D792 |
|
Kingfa MAC-601 UV PC/ABS Alloy
Features:Excellent balance propertiesHigh impact strengthGood processing propertiesApplications:Injection moldingAutomobile instrument panelElectrical and electronic partsComputer and accessoriesHou..
|
|||
| Specific Gravity | 1.13 g/cc | 1.13 g/cc | ASTM D 792 |
|
MRC Polymers NAXALOYâ„¢ 770-BK272 ABS + PC Alloy
Information provided by MRC Polymers Inc.
|
|||
| Specific Gravity | 1.13 g/cc | 1.13 g/cc | ASTM D792 |
|
SABIC Innovative Plastics SABIC STAMAX 30YM243 PP
SABIC® STAMAX 30YM243 is a 30% long glass fiber reinforced UV stabilized polypropylene. The glass fibers are chemically coupled to the PP matrix, resulting in high stiffness and strength. The IMD..
|
|||
| Specific Gravity | 1.13 g/cc | 1.13 g/cc | ASTM D792 |
|
Samsung Cheil Industries Starex® BF-0679P MABS, Unreinforced Scratch Resistant
Scratch resistant material that is used for the exterior material of flat TVInformation provided by Samsung Cheil Industries.
|
|||
| Specific Gravity | 1.13 g/cc | 1.13 g/cc | ASTM D792 |
|
Teknor Apex MONPRENE® MP 2730 Thermoplastic Elastomer
Information provided by Teknor Apex Company
|
|||
| Specific Gravity | 1.13 g/cc | 1.13 g/cc | ASTM D792 |
|
SABIC Innovative Plastics NORYL N190X PPE+HIPS (Asia Pacific)
PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. Dielectric strength. Suitable for E/E market applications.
|
|||
| Specific Gravity | 1.13 g/cc | 1.13 g/cc | ASTM D792 |
|
Lubrizol Estane® T470A Thermoplastic Polyurethane
Type: Estane® T470A is a Shore 77A, polyester grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Provided b..
|
|||
| Specific Gravity | 1.13 g/cc | 1.13 g/cc | ISO 1183/1 |
|
A. Schulman SCHULAMID® 6 MV14 Unreinforced Nylon 6
Information provided by A. Schulman.
|
|||
| Specific Gravity | 1.13 g/cc | 1.13 g/cc | |
|
A. Schulman SCHULAMID® 6 NV12 Easy Flow Low Viscosity Nylon 6
Information provided by A. Schulman.
|
|||
| Specific Gravity | 1.13 g/cc | 1.13 g/cc | ASTM D792 |
|
A. Schulman POLYBLAK™ 4669 Premium Conductive 35% Carbon Black Concentrate Based In LLDPE
DescriptionPOLYBLAK® Black 4669 is a premium conductive carbon black concentrate containing 35% carbon black based in LLDPE. This carbon black masterbatch is designed to provide smooth extruded su..
|
|||
| Specific Gravity | 1.13 g/cc | 1.13 g/cc | ASTM D792 |
|
A. Schulman POLYBLAK™ 3422 Black Color Concentrate, 35% Carbon Black Based In LDPE
DescriptionPOLYBLAK® Black 3422 is a black color concentrate containing 35% carbon black based in LDPE. This masterbatch is designed to provide excellent UV absorption with a regular brown underto..
|
|||
| Specific Gravity | 1.13 g/cc | 1.13 g/cc | ASTM D792 |
|
Lubrizol Estane® 2103-84AEN Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Contains UV Stabilizer, NSF Standard 61 certifiedAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pelletha..
|
|||
| Specific Gravity | 1.13 g/cc | 1.13 g/cc | ASTM D792 |
|
Eastman Neostar FN006 Elastomer
Neostar FN006 elastomer is the second in Eastman’s series of tough, clear, durable copolyester ethers. Developed for use in the profile and automotive markets, it can also be used in packaging and ..
|
|||
| Specific Gravity | 1.13 g/cc | 1.13 g/cc | |
|
Epoxy Technology EPO-TEK® E3035T-2 Electrically Conductive Epoxy
Product Description: EPO-TEK® E3035T-2 is a single component, silver-filled epoxy for semiconductor die attach, as well as SMD attach on hybrid circuits.Advantages & Application Notes: This epoxy c..
|
|||
| Specific Gravity | 1.13 g/cc | 1.13 g/cc | |
|
ChevronTexaco DEX-COOL® Extended Life Antifreeze/Coolant, Concentrate
FeaturesChevron DEX-COOL Extended Life Antifreeze/Coolant is a single-phase, ethylene glycol type universal automotive engine coolant based on a Chevron’s patented long life organic corrosion inhib..
|
|||
| Specific Gravity | 1.13 g/cc | 1.13 g/cc | ISO 1183 |
|
Azoty Tarnow™ Alphalon™ E 36 L Nylon 6
A bright polyamide 6 grade of medium viscosity that is suited for the production of films and monofilaments.Information provided by ATT Polymers™
|
|||
| Specific Gravity | 1.13 g/cc | 1.13 g/cc | ASTM D792 |
|
Asahi Kasei Thermylene® P6-30FG-0708 30% Glass Fiber Reinforced, High Impact
Information provided by Asahi Thermofil
|
|||
| Specific Gravity | 1.13 g/cc | 1.13 g/cc | catalyzed with Moldmaster Red |
|
ACC QM 2125 QSI Quantum Silicones 25 Durometer Condensation Cure Moldmaking Material
QM 2125 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent ch..
|
|||
| Specific Gravity | 1.13 g/cc | 1.13 g/cc | |
|
Momentive Performance Materials Silopren™ LSR 4060 Liquid Silicone Rubber - Healthcare
LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding ..
|
|||
| Specific Gravity | 1.13 g/cc | 1.13 g/cc | ASTM D792 |
|
A. Schulman POLYFORT™ FXP 3000-3120 Glass Sphere Filled Copolymer Polypropylene
DescriptionPolyfort® FXP 3000-3120 is a 30% glass sphere filled copolymer polypropylene compound.Information provided by A. Schulman.
|
|||
| Specific Gravity | 1.13 g/cc | 1.13 g/cc | ASTM D792 |
|
A. Schulman POLYBLAK™ 3422 Black Color Concentrate, 35% Carbon Black Based In LDPE
DescriptionPOLYBLAK® Black 3422 is a black color concentrate containing 35% carbon black based in LDPE. This masterbatch is designed to provide excellent UV absorption with a regular brown underto..
|
|||