Material Notes:
LEXAN FXM161R is a transparent/translucent medium viscosity grade for special effects colours with a metallic-luster appearance. Color package may affect performance.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.15 %
0.15 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.35 %
<br>@Temperature 23.0 °C
0.35 %
<br>@Temperature 73.4 °F
ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
on tensile bar; SABIC Method
Melt Flow 10 g/10 min
<br>@Load 1.20 kg,<br> Temperature 300 °C
10 g/10 min
<br>@Load 2.65 lb,<br> Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
Mechanical Properties Metric English Comments
Hardness, H358/30 95.0 MPa
13800 psi
ISO 2039-1
Tensile Strength at Break 70.0 MPa
10200 psi
50 mm/min; ISO 527
Tensile Strength, Yield 63.0 MPa
9140 psi
50 mm/min; ISO 527
Elongation at Break 60 %
60 %
50 mm/min; ISO 527
Elongation at Yield 6.0 %
6.0 %
50 mm/min; ISO 527
Tensile Modulus 2.35 GPa
341 ksi
1 mm/min; ISO 527
Flexural Yield Strength 90.0 MPa
13100 psi
2 mm/min; ISO 178
Flexural Modulus 2.30 GPa
334 ksi
2 mm/min; ISO 178
Taber Abrasion, mg/1000 Cycles 10
<br>@Load 1.00 kg
10
<br>@Load 2.20 lb
CS-17; SABIC Method
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
<br>@Temperature 23.0 - 80.0 °C
38.9 µin/in-°F
<br>@Temperature 73.4 - 176 °F
ISO 11359-2
Thermal Conductivity 0.200 W/m-K
1.39 BTU-in/hr-ft²-°F
ISO 8302
Deflection Temperature at 0.46 MPa (66 psi) 138 °C
280 °F
Edgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 127 °C
261 °F
Edgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 143 °C
289 °F
Rate B/50; ISO 306
145 °C
293 °F
Rate B/120; ISO 306
Flammability, UL94 HB
<br>@Thickness 3.00 mm
HB
<br>@Thickness 0.118 in
2nd value; UL 94 by SABIC-IP
HB
<br>@Thickness 1.10 mm
HB
<br>@Thickness 0.0433 in
UL 94 by SABIC-IP
Oxygen Index 25 %
25 %
LOI; ISO 4589
Glow Wire Test 850 °C
<br>@Thickness 1.00 mm
1560 °F
<br>@Thickness 0.0394 in
Glow Wire Flammability Index; IEC 60695-2-12
Optical Properties Metric English Comments
Transmission, Visible 80 %
80 %
transparent/translucent; thickness not quantified
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
IEC 60093
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
ROA; IEC 60093
Dielectric Constant 2.7
<br>@Frequency 50.0 - 60.0 Hz
2.7
<br>@Frequency 50.0 - 60.0 Hz
IEC 60250
2.7
<br>@Frequency 1.00e+6 Hz
2.7
<br>@Frequency 1.00e+6 Hz
IEC 60250
Dielectric Strength 17.0 kV/mm
<br>@Thickness 3.20 mm
432 kV/in
<br>@Thickness 0.126 in
in oil; IEC 60243-1
27.0 kV/mm
<br>@Thickness 1.60 mm
686 kV/in
<br>@Thickness 0.0630 in
in oil; IEC 60243-1
35.0 kV/mm
<br>@Thickness 0.800 mm
889 kV/in
<br>@Thickness 0.0315 in
in oil; IEC 60243-1
Dissipation Factor 0.0010
<br>@Frequency 50.0 - 60.0 Hz
0.0010
<br>@Frequency 50.0 - 60.0 Hz
IEC 60250
0.010
<br>@Frequency 1.00e+6 Hz
0.010
<br>@Frequency 1.00e+6 Hz
IEC 60250
Comparative Tracking Index 225 V
225 V
IEC 60112
Descriptive Properties Value Comments
Ball Pressure Test, 125°C +/- 2°C PASSES