Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOCOMP EC008 PEI (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyetherimide (PEI)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP EC008 PEI (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LNP* THERMOCOMP* EC008 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features include: Electrically Conductive.
Physical Properties Metric English Comments
Density 1.44 g/cc
0.0520 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.00010 - 0.00050 cm/cm

@Time 86400 sec
0.00010 - 0.00050 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0010 - 0.0050 cm/cm

@Time 86400 sec
0.0010 - 0.0050 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 211 MPa
30600 psi
5 mm/min; ISO 527
Elongation at Break 0.90 %
0.90 %
5 mm/min; ISO 527
Tensile Modulus 27.0 GPa
3920 ksi
1 mm/min; ISO 527
Flexural Yield Strength 286 MPa
41500 psi
2 mm/min; ISO 178
Flexural Modulus 22.2 GPa
3220 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 25.0 kJ/m²
11.9 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 214 °C
417 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Electrical Properties Metric English Comments
Surface Resistance 10 - 1000 ohm
10 - 1000 ohm
ASTM D257