| Category | Polymer , Thermoplastic , Nylon , Nylon 6 |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | LNP Konduit |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | SABIC Innovative Plastics LNP KONDUIT PX10322 PA 6 (Asia Pacific).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.47 g/cc | 0.0531 lb/in³ | ASTM D792 |
| Water Absorption | 0.42 % @Time 86400 sec |
0.42 % @Time 24.0 hour |
SABIC Method |
| Moisture Absorption | 0.0600 % | 0.0600 % | 23°C / 50% RH; ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0029 cm/cm @Time 86400 sec |
0.0029 in/in @Time 24.0 hour |
ASTM D955 |
| Linear Mold Shrinkage, Transverse | 0.0032 cm/cm @Time 86400 sec |
0.0032 in/in @Time 24.0 hour |
ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 51.0 MPa | 7400 psi | Type I, 5 mm/min; ASTM D638 |
| Elongation at Break | 0.80 % | 0.80 % | Type I, 5 mm/min; ASTM D638 |
| Tensile Modulus | 10.53 GPa | 1527 ksi | 5 mm/min; ASTM D638 |
| Flexural Strength | 75.0 MPa | 10900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
| Flexural Modulus | 10.5 GPa | 1520 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
| Izod Impact, Notched | 0.200 J/cm | 0.375 ft-lb/in | ASTM D256 |
| Izod Impact, Unnotched | 1.04 J/cm | 1.95 ft-lb/in | ASTM D4812 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 22.5 µm/m-°C @Temperature -40.0 - 40.0 °C |
12.5 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| 25.7 µm/m-°C @Temperature 40.0 - 120 °C |
14.3 µin/in-°F @Temperature 104 - 248 °F |
ASTM E 831 | |
| CTE, linear, Transverse to Flow | 38.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
21.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| 58.2 µm/m-°C @Temperature 40.0 - 120 °C |
32.3 µin/in-°F @Temperature 104 - 248 °F |
ASTM E 831 | |
| Specific Heat Capacity | 1.72 J/g-°C | 0.411 BTU/lb-°F | ASTM C351 |
| Deflection Temperature at 1.8 MPa (264 psi) | 183 °C @Thickness 6.40 mm |
361 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
| UL RTI, Electrical | 140 °C | 284 °F | UL 746B |
| UL RTI, Mechanical with Impact | 120 °C | 248 °F | UL 746B |
| UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
| Flammability, UL94 | V-0 @Thickness 1.20 mm |
V-0 @Thickness 0.0472 in |
UL 94 |
| Glow Wire Test | 800 °C | 1470 °F | IEC 60695-2-13 |
| 960 °C @Thickness 1.00 mm |
1760 °F @Thickness 0.0394 in |
IEC 60695-2-12 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | >= 1.00e+13 ohm | >= 1.00e+13 ohm | ASTM D257 |
| Dielectric Strength | 11.0 kV/mm @Thickness 1.00 mm |
279 kV/in @Thickness 0.0394 in |
in oil; ASTM D149 |
| Comparative Tracking Index | 511 V | 511 V | IEC 60112 |
| Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
| High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |