| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
|
SABIC Innovative Plastics LNP KONDUIT PX10322 PA 6 (Asia Pacific)
Thermally conductive mineral filled PA6 FR compound, with through-plane and in-plane thermal conductivity of 1.7 W/(m*K) and 4.7 W/(m*K) respectively, conforming to ASTM E 1461 test standard.
|
|||
| UL RTI, Mechanical without Impact |
140
°C @Thickness 1.50 mm |
284
°F @Thickness 0.0591 in |
UL746B |
|
Covestro Apec® DP9-9331 High-Heat Polycarbonate, General Purpose
(discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
|
|||
| UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
|
Lanxess Pocan® T 7331 POS151 700226 PBT + PET, 30% Glass Fiber
PBT + PET, 30% glass fibers, injection molding, improved surface finish, increased temperature peak load, UV stabilizedInformation provided by LANXESS.
|
|||
| UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
|
SABIC Innovative Plastics Valox® 325 PBT (Asia Pacific)
General purpose, unreinforced, improved processing. Applications like sprinklers and nozzles, pumps, door handle, tank covers, pens, pencils etc.
|
|||
| UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
|
SABIC Innovative Plastics Valox® 357 PBT (Asia Pacific)
PBT + PC, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures.
|
|||
| UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
|
SABIC Innovative Plastics Valox® 357M PBT (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
|
SABIC Innovative Plastics Valox® 357U PBT (Asia Pacific)
Unreinforced PBTP, UL94 V-0/5VA rated. Improved UV resistant version of VALOX 357. Nonblooming flame retardant.
|
|||
| UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
|
SABIC Innovative Plastics Valox® 457 PBT
6.5% GR PBT, UL94 V-0/5V.
|
|||
| UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
|
SABIC Innovative Plastics Valox® 457 PBT (Asia Pacific)
6.5% GR PBT, UL94 V-0/5V.
|
|||
| UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
|
SABIC Innovative Plastics Valox® 735 PBT
40% glass/mineral, excellent thermal performance/low shrink. Motorized heating appliances, adaptor rings, oven grills, etc. Black/natural only.This data was supplied by SABIC-IP for the Americas re..
|
|||
| UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
|
SABIC Innovative Plastics Valox® 771 PBT
35% mineral/glass reinforced flame retardant grade with a CTI performance level class of 0 rating. Applications which may see electrical arcing.
|
|||
| UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
|
SABIC Innovative Plastics Valox® CS860 PBT+PET (Asia Pacific)
30% glass reinforced PBT+PET blend. Color stable, FR. Housewares, appliances; iron skirt, oven trim/panels.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
|
SABIC Innovative Plastics Valox® DR48 - CS1049 PBT (Europe-Africa-Middle East)
VALOX DR48 is a 15 % glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot..
|
|||
| UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
|
SABIC Innovative Plastics Valox® DR48 PBT (Asia Pacific)
17% glass reinforced, flame retardant grade UL-94 rated V-0/5VA.
|
|||
| UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
|
SABIC Innovative Plastics Valox® DR51 PBT
15% GR polyester, excellent mechanical, thermal and electrical performance. Non-flame retardant. Spotlights, appliance housings, handles, connectors
|
|||
| UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
|
SABIC Innovative Plastics Valox® DR51M PBT (Asia Pacific)
15% GR; exc. mechanical/thermal/electrical performance; nonflame retardant. For spotlights, appliance housings, handles. Easy flow/int. mold release.This data was supplied by SABIC-IP for the Asia ..
|
|||
| UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
|
SABIC Innovative Plastics Valox® EF4530 PBT (Asia Pacific)
Easy flow, 30% glass-reinforced, PBTP resin. Flame retardant.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
|
SABIC Innovative Plastics Valox® EXVX0095 PBT (Europe-Africa-Middle East)
VALOX EXVX0095 will be GLOBAL 420SE0 per January 2009.
30% GF PBT Flame Retardant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
|
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Asia Pacific)
Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified.
|
|||
| UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
|
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Europe-Africa-Middle East)
Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified.
|
|||
| UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
|
SABIC Innovative Plastics Valox® IQ357M PBT+PC (Asia Pacific)
Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release.
|
|||
| UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
|
SABIC Innovative Plastics Xenoy® X3108UV PBT+PC (Europe-Africa-Middle East)
Unreinforced, UV-stabilized, flame retardant, impact modified PBT+PC with V0 at 0.8mm thickness. For interior and exterior applications like wall switches and electrical enclosures.This data was sup..
|
|||
| UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
|
SABIC Innovative Plastics LNP Thermocomp RF0057E PA 66 (Europe-Africa-Middle East)
LNP* Thermocomp* RF0057E is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. Added features of this material include: Non-Brominated & Non-Chlorinated Flame Retardant.Thi..
|
|||
| UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
|
SABIC Innovative Plastics Valox® 430 PBT (Asia Pacific)
33 % glass reinforced, impact modified. Connectors, etc.
|
|||
| UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
|
SABIC Innovative Plastics Valox® 451E PBT
20% GR. Easy flow version of VALOX 451.
|
|||
| UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
|
SABIC Innovative Plastics Valox® ENH3500 PBT (Europe-Africa-Middle East)
Unfilled PBT, Non-Brominated & Non-Chlorinated Flame Retardant
|
|||
| UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
|
SABIC Innovative Plastics Valox® EXVX1403 PBT (Asia Pacific)
33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE.
|
|||
| UL RTI, Mechanical without Impact |
140
°C @Thickness 1.50 mm |
284
°F @Thickness 0.0591 in |
746B |
|
BASF Ultramid® KR 4355 G5 25% Glass Filled PA6/6T (Dry)
Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r..
|
|||
| UL RTI, Mechanical without Impact |
140
°C @Thickness 2.00 mm |
284
°F @Thickness 0.0787 in |
UL 746B |
|
DuPont Performance Polymers Rynite® 530 BK503 PET
(Unverified Data**)
Rynite® 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength, stiffness, and toughness, excellent electrical properties, surface appearance, ..
|
|||
| UL RTI, Mechanical without Impact |
140
°C @Thickness 0.810 mm |
284
°F @Thickness 0.0319 in |
UL 746B |
|
DuPont Performance Polymers Rynite® 530 BK503 PET
(Unverified Data**)
Rynite® 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength, stiffness, and toughness, excellent electrical properties, surface appearance, ..
|
|||