Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Mineral Filled
Manufacturer Ravago Manufacturing Americas, LLC
Trade Name Hylon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ravago Manufacturing Americas Hylon® N1240MHL BK Nylon 6/6.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Available in North America Filler: Mineral, 40% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated, Low Warpage and Heat StabilizedRoHS CompliantForm: Pellets Processing Method: Injection Molding Color: BlackInformation provided by Ravago.
Physical Properties Metric English Comments
Specific Gravity 1.50 g/cc
1.50 g/cc
ASTM D792
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0070 - 0.010 cm/cm
0.0070 - 0.010 in/in
ASTM D955 and ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 84.8 MPa
12300 psi
ISO 527-2
86.2 MPa
12500 psi
ASTM D638
Elongation at Break 1.8 %
1.8 %
ASTM D638
Flexural Strength 13.8 MPa
2000 psi
ASTM D790
13.8 MPa
2000 psi
ISO 178
Flexural Modulus 7.17 GPa
1040 ksi
ISO 178
7.24 GPa
1050 ksi
ASTM D790
Izod Impact, Notched 0.374 J/cm
0.700 ft-lb/in
ASTM D256
Izod Impact, Notched (ISO) 3.57 kJ/m²
1.70 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 192 °C
377 °F
Unannealed; ASTM D648