Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 2.55 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.55 GPa
370 ksi
ASTM D790
PolyOne Geon™ Vinyl Rigid Molding M5200 Natural Polyvinyl Chloride, Rigid (PVC, Rigid)
NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of..
Flexural Modulus 2.55 GPa
370 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Cycoloy® EHA PC+ABS (Asia Pacific)
PC+ABS. Electroplateable.
Flexural Modulus 2.55 GPa
370 ksi
ASTM D790
Ravago Manufacturing Americas Hylac® HF143 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Flexural Modulus 2.55 GPa
370 ksi
2.0 mm/min; ISO 178
Phillips Sumika Marlex® CHN-200 Thermoplastic Polyolefin  (discontinued **)
Thermoplastic Polyolefin, High Stiffness, Talc-FilledApplications: Automotive InteriorsConditioning after Molding: 48 hr at 23°CNominal Shrinkage: 0.9-1.1%Drying conditionsTemperature: 80-100°CTim..
Flexural Modulus 2.55 GPa
370 ksi
ASTM D790
Kolon Kocetal® VT701 Modified Grade Acetal Copolymer  (discontinued **)
Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ..
Flexural Modulus 2.55 GPa
370 ksi
ASTM D790
LG Chemical LUCEL N109-HR Heat Resistant POM, Unreinforced, Standard Viscosity
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Flexural Modulus 2.55 GPa

@Thickness 6.40 mm
370 ksi

@Thickness 0.252 in
2.8mm/min; ASTM D790
LG Chemical LUCEL N109LD POM, Chemical Resistance
Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical
Flexural Modulus 2.55 GPa
370 ksi
23°C; 50%RH; ASTM D570
LG Chemical Lucet® N109 Acetal Copolymer
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Flexural Modulus 2.55 GPa
370 ksi
ASTM D790
Techmer ES Luriblend® PA6/12 01430 Nylon 612
Availability: North AmericaForms: PelletsAdditive: Molybdenum Disulfide LubricantFeatures: Lubricated, Low Friction and Good Wear ResistanceInformation provided by TP Composites, Inc.
Flexural Modulus 2.55 GPa
370 ksi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® EA-0640 ABS, Unreinforced
Permanent static prevention ABS material such as LCD carrierInformation provided by Samsung Cheil Industries.
Flexural Modulus 2.55 GPa
370 ksi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® LX-0957 ABS, Unreinforced Metallic-Look
Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries.
Flexural Modulus 2.55 GPa
370 ksi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® NH-1907 HIPS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Flexural Modulus 2.55 GPa
370 ksi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® SF-0950 MABS, Unreinforced Scratch Resistant
Information provided by Samsung Cheil Industries.
Flexural Modulus 2.55 GPa
370 ksi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Infino® HP-0500 ABS, Unreinforced Heat Resistant
ABS material that can mainly be used for the exterior material of household appliances etc.Information provided by Samsung Cheil Industries.
Flexural Modulus 2.55 GPa
370 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-KON DX02437 PC (Asia Pacific)
LNP Stat-Kon DX02437 is a compound based on Polycarbonate resin containing conductive carbon powder, with good impact-resistance, flow and ESD performance, suitable for semi-con industry.
Flexural Modulus 2.55 GPa
370 ksi
ASTM D790
Tipco Tipcolene® FPTC 30 HG - 30% Talc & Calcium Carbonate Polypropylene Homopolymer, High Gloss & Stiffness
30% Talc+Calcium Reinforced PP Homopolymer with High GlossApplications: Furniture & AppliancesProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Flexural Modulus 2.55 GPa
370 ksi
ASTM D790
Westlake Plastics Norylux™ EN-265 Modified Polyphenylene Oxide
Norylux modified PPO is a strong, engineering plastic with outstanding mechanical, thermal, and electric properties. Low moisture absorption and low thermal expansion make Norylux one of the most d..
Flexural Modulus 2.55 GPa
370 ksi
23°C, 50% RH; ASTM D790
Asahi Kasei Xyron® 640Z Modified Polyphenylene Ether
Flame RetardantInformation provided by Asahi Kasei
Flexural Modulus 2.55 GPa
370 ksi
ASTM D790
Aaron Industries AAROPRENE® CFIPP 2040 High Impact Calcium Carbonate Filled Polypropylene
AAROPRENE® CFIPP 2000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified.
Flexural Modulus 2.55 GPa
370 ksi
ASTM D790
Beijing Ranger Chem BLUESTAR® BS350 Acetal Copolymer
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Flexural Modulus 2.55 GPa
370 ksi
ASTM D-790
Axiall 2651 Rigid PVC, Molding
Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Flexural Modulus 2.55 GPa
370 ksi
ISO 178
Polyplastics Duracon® M270-45 Acetal Co-polymer (POM), Weather resistance, High flow, High cycle
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..