Polymer Property : Rear Barrel Temperature = 199 °C Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Rear Barrel Temperature 191 - 199 °C
375 - 390 °F
RheTech Products FRP255-01 Polypropylene Copolymer, Flame Retardant, Black
Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 191 - 199 °C
375 - 390 °F
RheTech Products FRP256-00 Polypropylene Copolymer, Flame Retardant, Natural
Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 191 - 199 °C
375 - 390 °F
RheTech Products FRp256-01 Polypropylene Copolymer, Flame Retardant, Black
Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 191 - 199 °C
375 - 390 °F
RheTech Products FRP257-01 32% Talc Reinforced Polypropylene Copolymer, Flame Retardant, Black
Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 191 - 199 °C
375 - 390 °F
RheTech Products FRP300-00 20% Talc Reinforced Polypropylene Copolymer, Flame Retardant, Natural
Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 191 - 199 °C
375 - 390 °F
RheTech Products FRP300-01 20% Talc Reinforced Polypropylene Copolymer, Flame Retardant, Black
Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 177 - 199 °C
350 - 390 °F
Oxford Polymers C-Acetal 25GF-BK Acetal, 25% Glass Fiber Reinforced
Product Description: Glass Fiber (25% Reinforced), Acetal Injection Molding Grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Glass FiberSpecial Characteristics: Pre-color..
Rear Barrel Temperature 177 - 199 °C
350 - 390 °F
Oxford Polymers C-Acetal -30GF-Natural Acetal Copolymer, 30% Glass Fiber Reinforced
Product Description: Glass Fiber (30% Reinforced), Co-polymer Acetal, Injection Molding Grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Glass FiberSpecial Characteristic..
Rear Barrel Temperature 191 - 199 °C
375 - 390 °F
Polymer Resources ABS-G5 ABS, 5% Glass Reinforced
Acrylonitrile Butadiene Styrene, 5% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information ..
Rear Barrel Temperature 179 - 199 °C
355 - 390 °F
Ravago Manufacturing Americas Hylac® GP74 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Rear Barrel Temperature 179 - 199 °C
355 - 390 °F
Ravago Manufacturing Americas Hylac® HF224 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Rear Barrel Temperature 191 - 199 °C
375 - 390 °F
Polymer Resources ABS-G15 ABS, 15% Glass Reinforced
Acrylonitrile Butadiene Styrene, 15% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information..
Rear Barrel Temperature 191 - 199 °C
375 - 390 °F
Polymer Resources ABS-G20 ABS, 20% Glass Reinforced
Acrylonitrile Butadiene Styrene, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information..
Rear Barrel Temperature 179 - 199 °C
355 - 390 °F
Ravago Manufacturing Americas Hylac® GP48 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Rear Barrel Temperature 182 - 199 °C
360 - 390 °F
Fiberfil® PP-61/VO Polypropylene Copolymer, Flame Retardant, UL94 V0
Information provided by FIBERFIL Engineered Plastics
Rear Barrel Temperature 177 - 199 °C
350 - 390 °F
Multibase Multi-Flex® D 3104-8 TPO Thermoplastic Polyolefin Elastomer
Features: Chemical Resistance, Good PaintableOzone Resistant Thermal Stability, GoodDensity, LowTear Strength, GoodScratch Resistant Forms:PelletsProcessing Method:Injection Molding Uses: Automot..
Rear Barrel Temperature 177 - 199 °C
350 - 390 °F
Multibase Multi-Flex® D 4502 TPO Thermoplastic Polyolefin Elastomer
Features: Chemical Resistance, Good PaintableOzone Resistant Thermal Stability, GoodDensity, LowTear Strength, GoodScratch Resistant Forms:PelletsProcessing Method:Injection Molding Uses: Automot..
Rear Barrel Temperature 177 - 199 °C
350 - 390 °F
Multibase Multi-Flex® D 5308 TPO Thermoplastic Polyolefin Elastomer
Features: Chemical Resistance, Good PaintableOzone Resistant Thermal Stability, GoodDensity, LowTear Strength, GoodScratch Resistant Forms:PelletsProcessing Method:Injection Molding Uses: Automot..
Rear Barrel Temperature 177 - 199 °C
350 - 390 °F
Multibase Multi-Flex® D 6606 TPO Thermoplastic Polyolefin Elastomer
Features: Chemical Resistance, Good PaintableOzone ResistantDensity, LowTear Strength, GoodUV Resistance, GoodStiffness, Good Forms:PelletsUses: Automotive ApplicationsInformation provided by Mul..
Rear Barrel Temperature 177 - 199 °C
350 - 390 °F
Multibase Multi-Flex® 1047-2000 TPO Thermoplastic Polyolefin Elastomer
Features: Chemical Resistance, Good PaintableOzone Resistant Thermal Stability, GoodDensity, LowTear Strength, Good Forms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsI..
Rear Barrel Temperature 177 - 199 °C
350 - 390 °F
Multibase Multi-Flex® D 3104 TPO Thermoplastic Polyolefin Elastomer
Features: Chemical Resistance, Good PaintableOzone Resistant Thermal Stability, GoodDensity, LowTear Strength, Good Forms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsI..
Rear Barrel Temperature 182 - 199 °C
360 - 390 °F
Teknor Apex Flexalloy® 9100-75 Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, General Purpose, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather..
Rear Barrel Temperature 188 - 199 °C
370 - 390 °F
Advanced Polymer Alloys DuraGrip™ DGR 6040 NC/BK Thermoplastic Elastomer (TPE)
DuraGrip® DGR 6040 NC/BK are designed to be general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR 6040 NC/BK have an excellent soft t..
Rear Barrel Temperature 188 - 199 °C
370 - 390 °F
Advanced Polymer Alloys DuraGrip™ DGR 6060 NC Thermoplastic Elastomer (TPE)
DuraGrip® DGR 6060NC is designed to be a general purpose Thermoplastic Elastomer (TPE) that is easy to use in injection molding and extrusion processes. DGR 6060NC has an excellent soft touch feel,..
Rear Barrel Temperature 188 - 199 °C
370 - 390 °F
Advanced Polymer Alloys DuraGrip™ DGR 6070 NC Thermoplastic Elastomer (TPE)
DuraGrip® DGR 6070NC is designed to be a general purpose Thermoplastic Elastomer (TPE) that is easy to use in injection molding and extrusion processes. DGR 6070NC has an excellent soft touch feel,..
Rear Barrel Temperature 177 - 199 °C
351 - 390 °F
Ineos Nova 8048 High Performance Styrenic Enhanced Polystyrene  (discontinued **)
Improved toughness, Custom colorsApplications: Designed for injection molding applications requiring clarity and toughnessPerformance grades of polystyrene are engineered to have specific properties..
Rear Barrel Temperature 177 - 199 °C
351 - 390 °F
Ineos Nova 817 High Performance Styrenic Enhanced Polystyrene  (discontinued **)
High flow crystal polystyrene, Custom colorsApplications: Injection molding, Designed for use in high speed, Thin section applications and complex parts designs where custom coloring is a requiremen..
Rear Barrel Temperature 191 - 199 °C
375 - 390 °F
Ravago Manufacturing Americas Hylac® GP30G ABS, 30% Glass Fiber Reinforced
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Rear Barrel Temperature 171 - 199 °C
340 - 390 °F
LTL Color Compounds ColorFast® FRPS100 Styrene, High Impact
V1-rated high impact styreneAll information provided by LTL Color Compounders, Inc.