Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Radici Radiflam® BN100 AE Polybutylene Terephthalate

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer Radici Group Plastics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Radiflam® BN100 AE Polybutylene Terephthalate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
PBT Self-extinguishing with halogenInformation provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.45 g/cc
1.45 g/cc
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.0 MPa
7980 psi
ISO 527-1/2
Elongation at Break 2.5 %
2.5 %
ISO 527-1/2
Tensile Modulus 3.10 GPa
450 ksi
ISO 527-1/2
Flexural Strength 90.0 MPa
13100 psi
ISO 178
Flexural Modulus 2.60 GPa
377 ksi
ISO 178
Charpy Impact, Notched 0.300 J/cm²
1.43 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 225 °C
437 °F
ISO 1135 7-1-3
Deflection Temperature at 0.46 MPa (66 psi) 160 °C
320 °F
ISO 75/2Bf
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ISO 75/2Af
Vicat Softening Point 180 °C
356 °F
ISO 306
Flammability, UL94 V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved