MV Labs V860 KVO3 Potassium metavanadate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs V860 KVO3 Potassium metavanadate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 138.04 g/mol
138.04 g/mol
Descriptive Properties Value Comments
Assay 37% V
CAS Number 13769-43-2
Form White crystals
Purity 99.99%
Typical Impurities Na < 10; Al = 4; Ca, Fe = 2; Ba, Mg < 1 ppm